Flux residue cleaning procedure

Electronics Forum | Mon Oct 30 20:24:35 EST 2006 | davef

As we understand it, you: * Get some nice BGA from your supplier * Find BGA to be packaged properly * Bake the BGA for 24 hours at [what temperature?] to reduce the potntial for damaging moisture sensitive components during following processes * Remo

baked on water soluble flux residue betwwen fine pitch comp.

Electronics Forum | Fri Dec 01 14:12:50 EST 2000 | Jim M.

My company currently uses water soluble paste for our SMT process. We were having trouble retaining hot water in our in line, closed loop DI cleaner. The cleaner kept shutting down when the water temp. dropped below 125C. As a result, the conveyor

Finding a white strand on fine pitch components

Electronics Forum | Fri Aug 28 05:07:59 EDT 2009 | sachu_70

Do you clean the stencil manually or using the automated under-stencil cleaner on your Printer (recommended)? 1. Ensure that stencil wipes are lint-free and soaked sufficiently with solvent before use. 2. If your printer supports automated cleaning

Removal of No-Clean flux residue

Electronics Forum | Fri Sep 07 21:43:40 EDT 2001 | mugen

Hi, We use IPA and Prozone, if IPA is so drastically detrimental, to the pcba's.....what suggested alternative, can you please recommend, as IPA replacement? Thanks.

White residue VS No clean

Electronics Forum | Sat Jul 28 05:31:20 EDT 2001 | nop_e

Hi all I just got feedback from my customer about "White residue problem" around solder joints with manaul soldered connector at customer site and included the failure analysis report that there is residues of Cl,S,Na . I 'd like to know, the whi

Re: White residue on PCB's

Electronics Forum | Thu Oct 12 17:56:58 EDT 2000 | DennisF

The white residue can be caused by putting Alcohol on the no clean product. Some people will attempt to clean an area they have reworked.

White powdery residue following Wave

Electronics Forum | Fri Mar 02 15:32:52 EST 2001 | jagman

We are seeing a white, powdery residue following the Wave process. Is this a solder masking issue (poor cure from the PCB mfg) or Wave process related? Any input is greatly appreciated.

White powdery residue following Wave

Electronics Forum | Tue Mar 06 13:59:39 EST 2001 | dason_c

I have experience to the Kester 2331 water soluble flux long time ago with white residue and it related to the solder masking. Check what kind of the solder mask and ask Kester to do the test for you. Rgds.

Re: White residue on PCB's

Electronics Forum | Wed Oct 11 10:29:28 EDT 2000 | G. English

Try the following steps : FIRST CHECK THE ARCHIVE for further information, it WILL help you. Step One : What�s the chemical analysis of this white res? Obtain a sample. It could be tin, rosin, or something else??? Step Two : The fastest way I know

Removal of No-Clean flux residue

Electronics Forum | Thu Sep 06 10:55:37 EDT 2001 | davef

saturation occurs at ppm levels. Remember, IPA is extremely flammable and its bulk use makes the plant liable to all sorts of quite repressive safety rules/regulations and so on. Ignoring these rules exposes the owner to fines and possible plant cl