Electronics Forum | Fri Oct 22 10:41:08 EDT 2010 | janz
hi 1) just run test batch and pull test wire. Use MIL std to find out your results. 2) again run through and test wire.
Electronics Forum | Wed Jun 17 14:46:18 EDT 1998 | Robert Smith
1. I need to be able to probe into my product's substrate which has all components in die form. I would need to be able to bring out any pad information for hookup to a scope or any other external piece of equipment. I do not have the convenience o
Electronics Forum | Mon Apr 26 11:04:53 EDT 1999 | Dave F
| | Earl said, in essence: | | | | | Justin is absolutely right ... | | | | | | Again, Entek is not much more than a flux coating ... | | | | | | Metallic coatings protect best, as we all know - especially those electroplated. Those coatings chemi
Electronics Forum | Mon Apr 26 17:45:26 EDT 1999 | Earl Moon
| | | Earl said, in essence: | | | | | | | Justin is absolutely right ... | | | | | | | | Again, Entek is not much more than a flux coating ... | | | | | | | | Metallic coatings protect best, as we all know - especially those electroplated. Those