Suspected Pink Ring

Electronics Forum | Tue Jul 27 11:59:19 EDT 1999 | Wolfgang Busko

While inspecting incoming PCBs we detected around all plated-through-holes (only there and all in the same place) some halfmoonshaped light rings that match obviously only with the pink ring symptom shown in the IPC-A-600 chapter 2.5.2.. That would m

Any PCB manufacturer can do 8 layer 1.0mm PCB with 2/2mil line?

Electronics Forum | Mon Jul 24 20:39:49 EDT 2017 | dawson

We got an inquiry from US that requires high > volume 8 layer 1.0mm PCB, OSP + selective ENIG > surface, 5 groups impedance control, and stacked > vias. These requirements are common, but there is > 2/2mil lines in inner layers. It's said that th

IDE PATA Connector

Electronics Forum | Tue Sep 14 01:43:25 EDT 2021 | kumarb

jane@szjiln.com&quot;>jane@szjiln.com">jane@szjiln.com/</a> <a class=roll href="mailto:janeszjiln@gmail.com">janeszjiln@gmail.com&quot;>janeszjiln@gmail.com">janeszjiln@gmail.com </a>Cell:+86-136325247

Re: Suspected Pink Ring

Electronics Forum | Tue Jul 27 17:47:36 EDT 1999 | Earl Moon

| While inspecting incoming PCBs we detected around all plated-through-holes (only there and all in the same place) some halfmoonshaped light rings that match obviously only with the pink ring symptom shown in the IPC-A-600 chapter 2.5.2.. That would

Re: Suspected Pink Ring

Electronics Forum | Wed Jul 28 20:14:22 EDT 1999 | Dave F

| While inspecting incoming PCBs we detected around all plated-through-holes (only there and all in the same place) some halfmoonshaped light rings that match obviously only with the pink ring symptom shown in the IPC-A-600 chapter 2.5.2.. That would

Re: Suspected Pink Ring

Electronics Forum | Wed Jul 28 12:02:48 EDT 1999 | Wolfgang Busko

| | While inspecting incoming PCBs we detected around all plated-through-holes (only there and all in the same place) some halfmoonshaped light rings that match obviously only with the pink ring symptom shown in the IPC-A-600 chapter 2.5.2.. That wou

Re: Suspected Pink Ring

Electronics Forum | Thu Jul 29 15:35:05 EDT 1999 | Earl Moon

| | While inspecting incoming PCBs we detected around all plated-through-holes (only there and all in the same place) some halfmoonshaped light rings that match obviously only with the pink ring symptom shown in the IPC-A-600 chapter 2.5.2.. That wou

Re: Suspected Pink Ring

Electronics Forum | Wed Jul 28 16:36:30 EDT 1999 | Earl Moon

| | | While inspecting incoming PCBs we detected around all plated-through-holes (only there and all in the same place) some halfmoonshaped light rings that match obviously only with the pink ring symptom shown in the IPC-A-600 chapter 2.5.2.. That w

Re: Suspected Pink Ring

Electronics Forum | Fri Jul 30 10:30:23 EDT 1999 | Wolfgang Busko

| | | While inspecting incoming PCBs we detected around all plated-through-holes (only there and all in the same place) some halfmoonshaped light rings that match obviously only with the pink ring symptom shown in the IPC-A-600 chapter 2.5.2.. That w

Re: Suspected Pink Ring

Electronics Forum | Fri Jul 30 16:06:22 EDT 1999 | Earl Moon

| | | | While inspecting incoming PCBs we detected around all plated-through-holes (only there and all in the same place) some halfmoonshaped light rings that match obviously only with the pink ring symptom shown in the IPC-A-600 chapter 2.5.2.. That

  1  

2.5.2 searches for Companies, Equipment, Machines, Suppliers & Information

Circuit Board, PCB Assembly & electronics manufacturing service provider

Training online, at your facility, or at one of our worldwide training centers"
Win Source Online Electronic parts

Have you found a solution to REDUCE DISPENSE REWORK? Your answer is here.
PCB Handling with CE

Component Placement 101 Training Course
PCB Handling Machine with CE

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.