Poor Solderability on TSOPs with Alloy 42 Leadframes

Electronics Forum | Wed Jun 22 09:42:51 EDT 2005 | davef

Not sure what a higher Tg laminate will accomplish. Can't hurt though. Remember, when soldering to Alloy 42, the surface is 42% nickel. So, you need to raise the reflow temperature some 15 to 20*C over what is needed for copper. Also, sometimes All

Pure Tin Quandry

Electronics Forum | Fri Jun 03 16:40:48 EDT 2005 | Andrea

I have a customer who has put a restriction against pure tin finish components. We have gotten our BOMs compliant with all but 5 parts. Fairchild p/n FDD6512A, FQD12N20C, IRLM120A Bournes 3214G-1-501E Sprague 10TS-D10 I am looking for a standard pr

High temp grease needed

Electronics Forum | Tue Aug 23 14:23:00 EDT 2005 | pjc

Most ovens I know use oil to lubricate conveyor chain, not grease. Anyway, is this what you're using: NMG No Melt Grease NLGI 2 (operates from -20�C to +270�C) NMG is a long-fibred highly adhesive grease which does not melt or drip at high temperat

ceramic cap cracking

Electronics Forum | Wed Feb 02 08:51:25 EST 2005 | Dougs

we have a capacitor cracking on one of our boards, there are four of the same cap on the board and only one cracks, we are seeing about 6% of the component cracking. it's not near the edges of the board and he board is 2.4mm thick so i dont think it

  1  

20c 2005 208v searches for Companies, Equipment, Machines, Suppliers & Information

2024 Eptac IPC Certification Training Schedule

Training online, at your facility, or at one of our worldwide training centers"
Selective Soldering Nozzles

High Throughput Reflow Oven
used smt parts china

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...
IPC Training & Certification - Blackfox

Have you found a solution to REDUCE DISPENSE REWORK? Your answer is here.
design with ease with Win Source obselete parts and supplies

PCB Reverse Engineering, Redesign, & Repair Services & Equipment