Electronics Forum: 20s-40s 220 220 (Page 1 of 35)

Zevatech Print-MAT 220

Electronics Forum | Wed Feb 09 14:48:30 EST 2005 | tinkergaloot

can anyone provide me with information on the operation of the Zevatech Print-MAT 220? Its a pretty basic machine, but my question relates directly to the squeegee blade setup and leveling the blades to the stencil. If you level the blades together

TO-220 Chip Package - Bridges

Electronics Forum | Thu Jun 13 02:20:43 EDT 2013 | mun4o

put the silk screen mask between pads.Add drain pads after TO220.

REFLOW PROFILE NEED HELP

Electronics Forum | Thu Aug 25 09:56:08 EDT 2005 | james

I ran a profile on a dummy board with no parts and the peak temp is 220. The 220 is just the temperature of the board of course. With that BGA on it, I am pretty sure it sucks up alot of the heat. Also I am looking at the profile and notice that i

Pb free BGA voids

Electronics Forum | Tue May 02 07:56:58 EDT 2006 | billyd

Yeah, that's what I'm doing now. I have it now peaking around 235, with about 70 sec. above 220C. (220C is the reflow temp, according to manufacturer. I've always used 217C for Pb free) Wish me luck. Thanks!

QFP144 soldering problem

Electronics Forum | Mon Sep 10 15:49:28 EDT 2007 | mun4o

Hi, the solder on the pad is not molt.Temperature of the leads is about 220*C( I change this T from 214 to 232) but result is same - solder is granular and not diffuse.I think the T on leads is not enough high,bu I can't increase because the max T on

Please HELP! TO220 Lead Forming

Electronics Forum | Mon Mar 24 10:02:44 EST 2003 | ksfacinelli

I have a board that has a few TO220 packages with the 5 lead style. The problem I am encountering is forming the the leads. The TO220 package needs a 90 degree bend with pins 2 and 4 staggered. I am "not" doing thousands but would like to find a co

Reflow Profiling

Electronics Forum | Tue Oct 26 13:45:19 EDT 2004 | vinod

Hi friends I am using Alpha Metal WS709 solder paste. I know the spec for this solder paste. It recommends straight ramp to 220 C at 0.9 degree/sec and TAL 75 sec.So I am looking between around 27-220 temp around 215 second. And time above 183 not to

Reflow Profiling

Electronics Forum | Tue Oct 26 13:45:23 EDT 2004 | vinod

Hi friends I am using Alpha Metal WS709 solder paste. I know the spec for this solder paste. It recommends straight ramp to 220 C at 0.9 degree/sec and TAL 75 sec.So I am looking between around 27-220 temp around 215 second. And time above 183 not to

Please HELP! TO220 Lead Forming

Electronics Forum | Mon Mar 24 17:26:39 EST 2003 | pjc

try http://www.electro-prep.com

Please HELP! TO220 Lead Forming

Electronics Forum | Mon Mar 24 19:08:51 EST 2003 | rdr

You could always make your own manual bender with shim stock etc...

  1 2 3 4 5 6 7 8 9 10 Next

20s-40s 220 220 searches for Companies, Equipment, Machines, Suppliers & Information

SMTAI 2024 - SMTA International

High Resolution Fast Speed Industrial Cameras.
Solder Paste Dispensing

Have you found a solution to REDUCE DISPENSE REWORK? Your answer is here.
IPC Training & Certification - Blackfox

Software for SMT placement & AOI - Free Download.
Voidless Reflow Soldering

Training online, at your facility, or at one of our worldwide training centers"