Electronics Forum | Wed Feb 23 22:38:28 EST 2005 | davef
We: * Cure 1B73 according to spec in a heat box, like a Blue-M * Clean nozzles [one set in use, one set being cleaned] in thinner in a bronson ultrasonic cleaner * Haven't evaluated coatings in years, but would do it according to J-STD-001C, Reqmnts
Electronics Forum | Fri Aug 14 09:40:59 EDT 2015 | jvalverde
Hello, I want to make a simple conformal coating machine, I think in a Cartesian robot with MACH3 software. My questions are about the G-Code for the program (the software to design: % open/close nozzle, the paths (trajectory), import the pcb fi
Electronics Forum | Wed Jan 24 09:34:38 EST 2024 | wintercurrants
The equipment of Specialty Coating Systems and PVA is both simple to operate and maintain. Since it's a spray booth, constant maintenance is required or you risk having a serious headache. Our conformal coating line includes a double-sided UV oven, a
Electronics Forum | Wed Mar 04 10:59:24 EST 2015 | jpierre
Hi first DS65 version is a specific dilution for dispensing machine, in this case the typical process is following: application of the conformal coating extraction of solvent (low extraction power is better)2minutes and drying the drying can be done
Electronics Forum | Thu Jan 30 07:27:00 EST 2003 | cnotebaert
As said earlier the best way is to cure it then discard. Is your material heat cure or moisture cure? If heat cured and you ahve a oven place the material in trays and heat cure and discard. If moisture cure leave the material in the container and ad
Electronics Forum | Wed Oct 01 10:57:53 EDT 2008 | blnorman
Oxford Instruments makes a device called the OSPrey 800 that measures OSP thickness on the pads. We took a look at it last year because we have one line that uses OSP. It is pricey, and that's why we didn't order one, but if you use a lot of OSP, m
Electronics Forum | Wed Feb 19 22:04:08 EST 2003 | davef
Blondie I've never heard of using palladium [Pd] for a ring. [Not that that means much.] See, here's a link to discussion on using Pd in jewlery: http://jewelry.about.com/gi/dynamic/offsite.htm?site=http%3A%2F%2Fwww.professionaljeweler.com%2Farchi
Electronics Forum | Tue Mar 10 22:16:56 EST 1998 | Steve Gregory
Jeremy, I'm gonna make a couple of assumptions by "reading in between the lines" of your email: 1. You're using no-clean paste. 2. This is only happening on the second side. You tell me if I'm wrong about this... First thing, if you're only experienc
Electronics Forum | Wed Jun 29 14:36:11 EDT 2005 | Steve
A customer of mine is using Chemtronics (Circuit Works) CW3300 Overcoat pen. This is an acrylic conformal coating. It cures at Room temperature. They need something similar that can be UV cured in a pen form. Any suggestions?
Electronics Forum | Thu Jul 03 17:29:42 EDT 2008 | mikesewell
Re: item 3 - there are ultrasonic thickness machines (Panametrics makes one) that can measure coating dry with a small transducer head. A little pricey for ones that measure reliably in the .003" +/- .002" range.