Electronics Forum | Sun Aug 21 01:13:18 EDT 2016 | habbycam
Issue fixed. Thank you
Electronics Forum | Mon Jul 31 15:10:18 EDT 2000 | Kevin Hamby
We are looking for a small wave or infared solder station to solder 4" X 8" flat, thru hole circuit boards, in small qty's. Do you have any suggestions? Sincerely, Kevin Hamby V.P. Tech. Engineering/Sales Intech Assembly Solutions 54900 Pine Crest
Electronics Forum | Thu Oct 19 16:10:44 EDT 2000 | John Thorup
Much has been said on this subject. Try a search of the archives for the terms "Phil Zarrow" and "surface tension". You'll likely find what you need.
Electronics Forum | Thu Oct 19 16:10:48 EDT 2000 | John Thorup
Much has been said on this subject. Try a search of the archives for the terms "Phil Zarrow" and "surface tension". You'll likely find what you need.
Electronics Forum | Tue Nov 26 08:51:52 EST 2019 | marwan
we're using the Balverzinn Cobar 390-RX-HT and it wery good for wave and selective soldering and he can support a verry high temperatures
Electronics Forum | Thu Oct 19 12:34:36 EDT 2000 | lwatson
I can't seem to find an article about the limiting mass of a SMT component on the solderside of a double-sided reflowed PCB. I'm pretty sure that Phil Zarrow did an article on this subject. It went something like the mass/land surface area?
Electronics Forum | Tue Dec 07 05:16:12 EST 2004 | kanwal324
We are using solder paste of Alpha Metals 390DH4. As per manufacturer guidelines the viscosity of paste after 1/2 hr. conditioning and after mixing in paste mixer,it shoule be between 800-1250KCP. Our customer is asking for viscosity to be maintained
Electronics Forum | Fri Nov 29 10:26:01 EST 2019 | marwan
flux my leave a white residues even after cleaning, when we want to select a flux for our Ersa Ecoslect we tryed a varity of fluxes (including the IF2005C) and we decide to use the Cobar 390-RX-HT because he gaved us the best results in soldering and
Electronics Forum | Fri Dec 27 02:11:31 EST 2019 | anteiv
Hello, We are having problems with SMD wave soldering (ERSA) used flux is BALVER ZINN 390-RX-HT https://www.balverzinn.com/tl_files/balverzinn/downloads/intern/TDB/PDS_390-RX-HT_EN.pdf https://www.balverzinn.com/tl_files/balverzinn/downloads/datenb
Electronics Forum | Fri Jul 17 12:49:33 EDT 1998 | Aaron Delfausse
We currently use an ESP RMA paste. The reason that I initially posted the question was because we are conducting tests to see if this is infact the best paste for our processes. In running tests, however, certain variables, such as humidity, are ou