Electronics Forum: 600 smd (Page 2 of 4)

Omega Meter SMD 600 Ionograph

Electronics Forum | Tue Jan 15 14:19:55 EST 2008 | aqueous

Specialty Coating Systems: (800) 356-8260 (317) 244-1200 http://www.scscoatings.com/parylene_equipment/omegameter.aspx Good Luck! Mike Konrad Aqueous Technologies www.aqueoustech.com konrad@aqueoustech.com

Electromigration Testing

Electronics Forum | Tue Aug 31 13:16:23 EDT 2004 | GS

Hi Davef, if by using Omegameter 600 SMD I am reading 1,56 microgram NaCL/sqcm, what is the real value I am measuring? considering the 14 sensitivity ?

Ionic testing and No-Clean flux

Electronics Forum | Fri Feb 04 09:23:21 EST 2000 | Casimir Budzinski

If No-Clean flux does not need to be cleaned, then why do I get readings of up to 27(ug NaCl/sq in) on boards that are not washed, up to 23.4(ug NaCl/sq in) on boards washed with DI water only and from 1.2 to 10.1(ug NaCl/sq in) on boards washed with

Re: Water Batch Cleaners

Electronics Forum | Mon Jun 28 13:34:06 EDT 1999 | Scott Cook

| Hey Scott, | | Good posting. However, what test did you perform and what was the nature of your technology? Both ionics (SMD600) and SIR on RF product to the 3 Gig range. Power amps and Xceivers. Technology was mixed; double sided SMT. My bare b

Ionic - MIL-P-28809A vs IPC TM650 (2.3.25C)

Electronics Forum | Thu Nov 20 04:00:36 EST 2008 | caerleon

Our sub-contractors will be using SMD600. Thankyou all for your replies much appriciated.

Ionic - MIL-P-28809A vs IPC TM650 (2.3.25C)

Electronics Forum | Wed Nov 19 06:02:22 EST 2008 | caerleon

Hi all, I have been in the game for near on 15 years and finally something has stumped me! As this site has always provided a wealth of knowledge and at times some amusement I have decided to post it here. Ok. My company uses a test method on an Om

Electromigration Testing

Electronics Forum | Sat Sep 04 06:25:07 EDT 2004 | GS

Many Thanks Dave for your patience (GBY). I was just trying to give a chance to our connector Supllier to read few micrograms less of NaCl found with the connectors. But even if using a "bonus formula" they are out of specs. Following it could be i

IONIC CLEANLINESS SPEC FOR BARE PWBs

Electronics Forum | Sun May 09 16:25:00 EDT 2004 | gabriele

Military and most commercial standards requires > post-soldered boards to measure less than 10 > �g/in of NaCl (14 when using an Omegameter, 20 > on a Ionagraph, and 37 on a Zero-Ion). > > As Dave > stated, 6.5 �g/in of NaCl is called out in >

SMD flatness standard

Electronics Forum | Sat Nov 18 08:42:11 EST 2006 | davef

Bow & twist: IPC-A-600. Acceptability of Printed Boards 1.5%; Goal 0.005" per inch; Practicle 0.007" per inch

SMD flatness standard

Electronics Forum | Sat Nov 18 21:20:58 EST 2006 | Fer

Dave, May I ask where did you find the 1.5%, or the goal of .005" (or .007") per inch? The IPC-A-600 bow and twist standard calls for a .75% based on the calculation of the test method TM-650, method 2.4.22, which calculates the percentage based on


600 smd searches for Companies, Equipment, Machines, Suppliers & Information

Best SMT Reflow Oven

High Throughput Reflow Oven
pressure curing ovens

Training online, at your facility, or at one of our worldwide training centers"
High Throughput Reflow Oven

Stencil Printing 101 Training Course
convection smt reflow ovens

World's Best Reflow Oven Customizable for Unique Applications


"回流焊炉"