Electronics Forum: acrylic bubbles (Page 1 of 1)

1B73LOC Conformal Coating

Electronics Forum | Mon Jun 25 11:55:47 EDT 2007 | ck_the_flip

I don't think THEY (Humiseal) know how their material cures. I have a data sheet from them for 1B73, and it says 24 hours at room temperature or 30 min. @ 170�F. We use our in-line oven mainly to dry the material and make it tack-free. You would

Coating Brush Touch-up

Electronics Forum | Tue Dec 02 14:31:48 EST 2008 | dontfeedphils

Hey guys, just joined the site and I'm looking for some help. In our coating department we are running a Asymtek C-740 with a Jet and film coater. The coating that we are using is Humiseal 1B73 acrylic. The problem that we are having is that the C

Bubbles on solder joint(after conformal coating curing)

Electronics Forum | Fri Dec 18 09:07:24 EST 2009 | tommyg_fla

dave, where I work they are having the same problems with 1B31 acrylic. The coating thickness is 6-8 mils dried so that have to do several passes with an air dry between them and a final oven cure. They think that it might be related to the heating r

Re: Adhesion of conformal coating to plastic components

Electronics Forum | Wed Jun 03 07:13:27 EDT 1998 | Tom Tellinghuisen

| We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not al

Re: Conformal Coating

Electronics Forum | Fri Mar 20 10:31:19 EST 1998 | Mick Jones

| I will be starting a conformal coating process soon, I am looking for any pointers on | 1) Best method for masking components, tape mask, liqued mask | 2) Which is best Spray or Dip? | 3) Compatiblity with no clean solder paste (flux residue) | I h

Re: Adhesion of conformal coating to plastic components

Electronics Forum | Wed Jun 03 15:22:12 EDT 1998 | Greg Curler

| | We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not

Dymax vs Humiseal Urethane Confomals.... Anyone?

Electronics Forum | Tue Feb 03 13:39:08 EST 2009 | grics

Good morning Jamie. I work at a CM and can offer some input on process flexability. I do not have any data on how reliable the coating is but I can say that they are both very difficult to control. Will you be selective coating or full coating? Ho

  1  

acrylic bubbles searches for Companies, Equipment, Machines, Suppliers & Information

Void Free Reflow Soldering

High Throughput Reflow Oven
See Your 2024 IPC Certification Training Schedule for Eptac

Best Reflow Oven
PCB Handling Machine with CE

Training online, at your facility, or at one of our worldwide training centers"
Win Source Online Electronic parts

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...