Electronics Forum | Wed May 08 14:24:22 EDT 2013 | wahahasteven
we are using acrylic conformal coating on the PCB. Under the same program, same parameters (not changing anything on the machine), and we always found one or two boards have some spots which are not coated (shown as picture). The location of the spot
Electronics Forum | Mon Dec 27 10:03:35 EST 2010 | duso02
Contact your distributor for the coating or Humiseal directly. Humiseal has had a recent issue with batches of 1B31. The specific problem is lack of adhesion, which is what you have as well. You need to find out if your batch # is one of the affected
Electronics Forum | Sun Dec 26 23:48:01 EST 2010 | raghu
Dear Sir, We are using 1B31 conformal caoting of 48 sec viscosity in Zahn #1 cup, by machine(PVA354) application with Tank air pressure 2.3 psi, automising air pressure 1 psi. 7 days after application we are observing peeling off problem.. And n
Electronics Forum | Thu May 09 13:49:24 EDT 2013 | davef
First, it appears that your solder mask and your coating material appear to be incompatible. Second, IPA leaves a residue that's probably not compatible with your coating material, either. IPC-HDBK-830 - Guidelines for Design, Selection and Applic
Electronics Forum | Thu May 09 10:12:08 EDT 2013 | wahahasteven
this is one of my project. I have tried to remove coating only on those areas with alcohol and thinner, then program the machine to coat the removed area again. But the result obviously shows that two different tones of coating on the board. I also
Electronics Forum | Wed May 08 20:14:24 EDT 2013 | davef
What happens when you rework those non-coated areas? Please list your rework steps Br, davef
Electronics Forum | Mon Jan 03 00:30:30 EST 2011 | raghu
Contact your distributor for the coating or > Humiseal directly. Humiseal has had a recent > issue with batches of 1B31. The specific problem > is lack of adhesion, which is what you have as > well. You need to find out if your batch # is one >
Electronics Forum | Fri Nov 21 18:56:41 EST 2003 | jsloot
Gun wash is another term used for acrylic laquer thinner. We use DuPont 3642SC. We have much success in its use.
Electronics Forum | Thu Sep 10 15:01:28 EDT 2009 | mefloump
I currently spray DOW 2620 with my PVA650 without any problems. I do not thin it but I do have a distance between the coating machine and IR oven to provide a flash off period. I notice bubbles only when the flash off time is too short and the coatin
Electronics Forum | Wed Sep 02 11:36:22 EDT 2009 | kpm135
Is this an established process that is just now exhibiting these problems, or is this a brand new process you're just setting up? What is the rest of your process like? What is done to the boards before you coat them? Water washed? Solvent washed? Sa