Hey, I thought you were in the BIG house on some trumped-up tax rap. We use many RF shields each month. Generally, the shields are not plated and made of alloy 770 (or alloy 752), half hard temper, as the base material. * Alloy 770; 55%Cu, 27%Zn,
Electronics Forum | Sat Jun 04 12:11:49 EDT 2011 | davef
Q1) How to identify on good or bad RF shield that could contribute to dewetting? A1) We use Alloy 770 and 752 [German silver] for our RF shields. We have never seen a solderability issue, even aged stock solders well. * Nickel Alloy 752, Nickel Silv