Electronics Forum | Tue Jun 07 12:07:30 EDT 2016 | wlsmt
Sorry davef. I was not being clear. PCBAs came out cold soldered after being reflowed the first time with ALPHA WS-820. The flux gel ALPHA WS 609 was supposed to be applied only onto the terminations of caps where ALPHA WS-820 was for a second refl
Electronics Forum | Wed Jun 15 10:38:41 EDT 2016 | laynefelix
Hi everyone..i am new here. I am hardware design engineer and as per my experience PCBAs came out cold soldered after being reflowed the first time with ALPHA WS-820. The flux gel ALPHA WS 609 was supposed to be applied only onto the terminations of
Electronics Forum | Mon Jun 06 12:51:17 EDT 2016 | wlsmt
My operator applied flux gel ALPHA WS-609 on MG P/N FTH101XAP (CAP ALUM 100UF 50V 20% SMD) before aqueous washing the PCBAs. Solder paste used was ALPHA WS-820. Now the caps have yellow stains. Any solution to this is appreciated. Tks
Electronics Forum | Mon Jul 16 21:29:03 EDT 2001 | davef
Cleaning RMA with water is bad news. It will turn your solder connections white and remove none of the RMA residues. There was a thread on removing RMA within the past two weeks on SMTnet. Check the fine SMTnet Archives. Additionally, look at M
Electronics Forum | Thu Nov 17 20:51:16 EST 2005 | cangly
Morning Mike, We use Pb63/Sn37, Alpha Metal alloy. Solder pot is at 250 C. The profile of board after Preheat about 100 C, Lambda Wave about 220C (use both Lambda and Chip wave), DWell time 2.1s ~ 3s. Conveyor speed 1.5 in/min. We run by bare board a
Electronics Forum | Thu Mar 06 17:02:40 EST 2003 | Kris
Try alpha fry technologies. http://www.frymetals.com/manufacturing/solder_reclain1.html
Electronics Forum | Tue Apr 19 15:01:03 EDT 2011 | rdoss
Not sure who you've already looked at, but i know Alpha Metals has preforms.
Electronics Forum | Tue Apr 13 13:22:15 EDT 2004 | babe
Try another solder paste manufacturer. Aim out of Rhode Island, Alpha and or Kester. I'm sure that they will be of better assistance than the current supplier. Good Luck
Electronics Forum | Tue Apr 13 14:56:51 EDT 2004 | russ
in a thread titled ".5mm bga" there is a reference to a paste by alpha that is no-clean and is supposed to be made specifically for this situation. I suppose that increasing the pad dimension to .012" is out of the question? Russ
Electronics Forum | Fri Mar 22 14:19:38 EDT 2019 | gregcr
Thank you ProcEng1 Nordson sent me a flux suggestion list: No Clean: 1. Kester Select 10 2. ALPHA EF-2210 3. AIM FX-16 Water Sol: KESTER 2331-ZX Nozzle Tinning: SUPERIOR #75