Electronics Forum | Wed Sep 01 14:31:22 EDT 1999 | Dave F
| To aid in heat dissipation of our PCB, we would like to try having copper fill areas on the board that are hot air levelled and not covered with solder resist. Then, when the board is reflowed, solder paste would be applied and then solder. Has any
Electronics Forum | Thu Sep 02 04:26:02 EDT 1999 | Wolfgang Busko
| | To aid in heat dissipation of our PCB, we would like to try having copper fill areas on the board that are hot air levelled and not covered with solder resist. Then, when the board is reflowed, solder paste would be applied and then solder. Has a
Electronics Forum | Thu Oct 21 02:31:27 EDT 2010 | rok
OGER 4003C bounding to Aluminum I am hoping someone might have the solution to my problem I have the following PCB: RO4003 Thickness: .2mm Layer: top single/ bottom ground plane Finish: silver top and bottom .2um Size: 3mmx6mm I need to bound/groun
Electronics Forum | Wed Jul 22 06:58:50 EDT 2015 | migliore
Hi, I got the answer from edaboard.com A standard 6-layer stack is using 2 cores. Manufacturing steps for standard 6-layer are: 1. Etch both (double side) core substrates 2. Assemble, press and cure the complete stack: - copper foil - prepr
Electronics Forum | Tue Sep 26 07:46:49 EDT 2023 | robertanderson
A transformer winding machine is a specialized piece of equipment used in the manufacturing of transformers. Transformers are electrical devices that transfer electrical energy between two or more circuits through electromagnetic induction. They cons
Electronics Forum | Fri Dec 11 15:53:50 EST 2009 | smt_guy
Hi All, I have a PCB that is bonded on an aluminum plate. The size of PCB is 11" x 8" and 0.065" Thick, The aluminum plate has the same size and thickness as the PCB. Process is Lead Free. Questions: Is it possible and achieveable to bond the PC
Electronics Forum | Wed Feb 15 07:52:26 EST 2006 | cyber_wolf
Can anyone tell me where I can get aluminum tape for holding down thermo couples on PCB's ? Thanks
Electronics Forum | Fri Mar 19 16:13:00 EDT 2010 | davef
The aluminum material is typically plated by a zincation process, followed by nickel plate and a gold flash layer. What do the soldered side of the component and the soldered side of the aluminum coin look like? Do they both take solder?
Electronics Forum | Mon Jan 27 18:15:39 EST 2020 | slthomas
I have to ask this because "Material is applied over bare aluminum" doesn't make sense to me. Is that some kind of electrically insulative black anodization on the board surface? Because if it's just bare aluminum, how is the entire circuit not sho
Electronics Forum | Mon Apr 16 09:01:18 EDT 2007 | Steve
The best station I've ever worked with is a focused IR station from PDR. The station that I had was called a; "Lightmaster Pro". They have a different model name now, but you can see a datasheet for it at: http://www.pdr.co.uk/Datasheets/PDRX410-IR-
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830