Electronics Forum | Wed Dec 05 23:34:32 EST 2012 | aqueous
Typical conveyor speeds on leaded alloys and OA flux is 2 FPM. Typical conveyor speeds on lead-free alloys and OS flux is 0.5 FPM. Temperature should be 140 F. Most polypropylene inlines cleaners should not exceed 140 F. -Mike Konrad Aqueous Technol
Electronics Forum | Wed Sep 12 00:18:19 EDT 2018 | aqueous
Here's a link to an article regarding foam mitigation techniques. It my be helpful. There are many causes of foam. Water alone does not foam. Flux, solubilized in to the water can produce foam. Defluxing additives contain defaming agents which should
Electronics Forum | Thu Nov 21 11:10:07 EST 2013 | luciano
Hello, We've just started using VIGON A200 in our Aqueous Trident XLD system and observed that aluminium electrolytic capacitors get corroded. Concentration was set at 20% and washing is done by spray at 150F for 6 to 8 minutes. Then is rinsed seve
Electronics Forum | Wed Jan 08 12:10:29 EST 2014 | mlevesque
Hello everyone!! We are looking for a new PCB batch cleaner and I want know what is the best machine in the market according to you. WE have an AAT Aquatherm 9200 and it's a big crap, the machine is always broken. Aqueous Trident seems to be inter
Electronics Forum | Fri Mar 12 01:51:45 EST 2021 | proy
Resolved, the centrifugal pump seal (5/8th shaft) had failed and we were able to get a goulds replacement, back up and running in 2 days. Just FYI for anyone with similar problem in the future
Electronics Forum | Fri Feb 19 21:58:02 EST 2021 | proy
We have a AQ Trident which has been running quite well and we are very happy with it. Today - it started to leak where the main pump motor shaft goes into the impeller chamber - cannot see, but the liquic is coming out where the motor nests up agains
Electronics Forum | Thu Oct 28 11:50:11 EDT 2010 | phase1
We are having a little trouble with what appears to be a crystalization between our fine pitch parts. The problem appears after a a thourough wash of the pcb when dry. It looks like lead wiskers/haze between the joints.We are using water soluable lea
1 |