Electronics Forum | Fri Dec 18 12:45:23 EST 2015 | deanm

Using a vapor degreaser with a solvent such as Vertrel, Novec, Techspray 1655, Solstice, etc. may work for you but solvents can attack certain plastics. Should be fine for SMT though. This is assuming you are using a no-clean (RMA) type flux, not wat

Baking SMT Components

Electronics Forum | Thu Jul 17 13:57:21 EDT 2008 | dphilbrick

The recommended bake temperature for components in Tape and Reel is 40C. If you use a bake temperature higher than that, the cover tape and other elements of the packaging will degrade to the point that it becomes impossible to reliably use an automa

Humidity bake bends leads

Electronics Forum | Fri Apr 16 09:40:04 EDT 1999 | Gerry G

While trying to sell me a low temperature baking system for SMDs the salesman mentioned that the 125C for 24hr bake had been known to cause co-planarity defects. I thought I'd ask some experts. Any help guys?

SMD Moisture Sensitive Devices - Baking using vacuum-bake oven - seeking clarification

Electronics Forum | Fri Nov 01 08:39:43 EDT 2019 | johnce

At this point, I do not plan to back-fill with nitrogen. I have confirmed that vacuum baking, with the temperature set to 40°C, will result in the chamber %RH being less than 5%.

PCB BAKING

Electronics Forum | Tue Mar 17 10:47:56 EDT 2020 | davef

IPC-1601 covers PWB bake-out, methods for determining optimum bake time and temperature, caveats for certain PWB plating finishes, etc. IPC-1601 is to bare boards as J-STD-033 is to components

Component Baking

Electronics Forum | Thu May 21 11:30:59 EDT 1998 | Mike Glenn

Does anyone know about low pressure/low temperature ovens used for baking of moisture senstive components? Thanks

PCB Baking after Wash

Electronics Forum | Thu Dec 04 00:22:11 EST 2008 | maacolomer

Hi Steven, The 24 hrs bake is an overkill according with various J-STDs. Assuming a bake temperature over the 100 Celsius degrees. There are several factors to be considered before deciding the best methodology to wash misprinted board. However,

Re: Bakeing

Electronics Forum | Mon Nov 27 17:39:37 EST 2000 | Dave F

Daniel: In response to your questions: * Moisture level (wt%) that may cause delamination in PCB�s. - Certainly, it depends, but 100% moisture will not cause delamination of a PCB. [Now, heating that water is another question, isn�t it? ;-)] *

Re: Humidity bake bends leads

Electronics Forum | Sun Apr 18 03:58:26 EDT 1999 | P.L. Sorenson - Technical Consultant

| While trying to sell me a low temperature baking system for SMDs the salesman mentioned that the 125C for 24hr bake had been known to cause co-planarity defects. | I thought I'd ask some experts. Any help guys? | To remove moisture from low quanti

Baking MSL components in vacuum.

Electronics Forum | Tue Jan 09 08:46:03 EST 2018 | pavel_murtishev

Hi, "Baker with controlled humidity 5%" is actually dry cabinet. Using of dry cabinets i.e. ambient temperature baking is preferred. Vacuum will always be better. If you are going to use vacuum chamber, that will be the best method in my opinion.