Electronics Forum | Wed Nov 29 00:43:45 EST 2006 | callckq
Dear all, Recently, we run 2 models with heat sink attachment on top of this BGA(on top of this BGA, there is flip chip attached at the center of the BGA). Hence, the center of the BGA is higher than corner/side. We used conventional way to attach
Electronics Forum | Thu Sep 12 10:45:29 EDT 2002 | pbarton
We have used a laser cut stencil 0.15mm (0.006") thick with 0.3mm (0.012") square apertures radiused in the corners 0.06mm (0.0025") to aid paste release. This approach with the (type 3) paste we use has proven successful on thousands of devices plac
Electronics Forum | Thu Mar 30 21:46:56 EST 2000 | Dave F
Reg: This is copy / paste from draft version of IPC 7095 ( issued May 1999 ) ... 7.3 Assembly accept/reject criteria 7.3.1 Voids in solder joint a. Sources of Voids There can be voids in solder balls, or at the solder joints to the BGA, or at the so
Electronics Forum | Wed Sep 02 08:44:50 EDT 1998 | Kelly Morris
| Hi, | We are having problem with yield loss due to electrical fail. Further investigation shows that the failure is due to solder bridging under BGA. Has been there any study or experience on how this could occur and what we can do to prevent it.
Electronics Forum | Wed Nov 11 10:08:38 EST 1998 | Magnus
| | Hi, | | We are having problem with yield loss due to electrical fail. Further investigation shows that the failure is due to solder bridging under BGA. Has been there any study or experience on how this could occur and what we can do to prevent
Electronics Forum | Mon Jul 12 09:13:08 EDT 1999 | Mark Charlton
I need some advice concerning reflow of a BGA-292. Since I am not ready to change my entire process to no-clean, I decided to place the lone BGA-292 on a proto run using our BGA re-work station. The pcb is a moderately dense, single-sided, 8-layer
Electronics Forum | Sat Oct 28 02:25:19 EDT 2006 | mika
Agree!! Where is Your thermocouple-probes attacded and can we get the info from this? Delta-T of the comp. is very, very important! The single most important smt-process step is the profiling/recipy and as a result of this, this poor package will cor
Electronics Forum | Tue Apr 26 16:00:08 EDT 2005 | jdumont
Good day all, we are having problems with some new BGAs that are slowly filtering their way into our designs. Engineering really wants to use them and I am pressured to make them work. They are 54 ball BGAs. The pitch is .8 mils and the ball diameter
Electronics Forum | Mon Jul 12 12:39:39 EDT 1999 | M Cox
| I need some advice concerning reflow of a BGA-292. Since I am not ready to change my entire process to no-clean, I decided to place the lone BGA-292 on a proto run using our BGA re-work station. The pcb is a moderately dense, single-sided, 8-laye
Electronics Forum | Mon Jul 12 12:28:10 EDT 1999 | Wolfgang Busko
| I need some advice concerning reflow of a BGA-292. Since I am not ready to change my entire process to no-clean, I decided to place the lone BGA-292 on a proto run using our BGA re-work station. The pcb is a moderately dense, single-sided, 8-laye
Main Products: 1. Original new and Original Used SMT/AI Spare Parts. 2. SMT Equipments And Related Machine( SMT Calibration, SMT Feeder Carts,Conveyer etc.) 3. Maintenace and Repair Service Pre-Sales Service Provide details ab
Manufacturer's Representative / Manufacturer / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
3 Road Xintang, Fuhai Street,Fuyong
Shenzhen, 30 China
Phone: 13713862102