Solder joint dewetting or non wetting

Electronics Forum | Wed Nov 06 03:51:28 EST 2013 | cuperpeter

Hi rob, Thank you very much for your response. Profiling was made exactly on the pad, which showed dewetting, so the values are mentioned for this pad. PCB's is about a week old. It is possible that the surface of pads is already oxidized? I will t

solder joint problem

Electronics Forum | Fri Jul 26 08:25:25 EDT 2013 | emeto

If there is a way to pre-tin the parts, that might help in forming better joint with gold.

solder joint appearance

Electronics Forum | Thu Jul 29 21:11:13 EDT 2004 | davef

Could be lots of things. With limited information about temperatures, solder alloy, and cleaning; we'll swing for the fence that you got these solder connections very hot. So hot that Pb oxide is dominating the solder joint surface instead of the

SMD solder joint calculation

Electronics Forum | Terry Burnette |

Wed Jan 16 15:21:48 EST 2002

solder joint problem

Electronics Forum | Fri Jul 26 05:14:38 EDT 2013 | anilw2006

We had a solder joint problem in gold plated PLCC68 ic. We do double sided reflow process with Cookson OL107F paste. First we do top with paste and second with glue process.The solder joint shape and wetting looked normal.In the process of testing

Reliability of solder joint

Electronics Forum | Thu May 26 21:09:01 EDT 2005 | thaqalain

The reliability of a Gullwing component solder joint is in question when insufficient solder is evident: *at the heel of the lead *at the toe of the lead *none of the above

SMD solder joint calculation

Electronics Forum | Wed Jan 16 11:20:52 EST 2002 | bentzen

Hi... We tend to do a lot of footprint calculating for new SMD components. But what about the amount of solder paste on the solder pads. The amount of solder alloy is of cause determined by the stencil aperture size, stencil thickness and the sold

SMD solder joint calculation

Electronics Forum | Wed Jan 16 12:04:45 EST 2002 | dason_c

You can use the IPC-7525, Stencil Design Guidelines for start up.

solder joint problem

Electronics Forum | Mon Jul 29 05:48:35 EDT 2013 | anilw2006

Thanks for support. Is it any special process of pre-tinng? Regards, Anil wagh.

solder joint appearance

Electronics Forum | Tue Jul 27 13:48:45 EDT 2004 | Ralf

Hi Recently i have noticed that after reflow (hot air oven) on the solder lands without components but with solder(screen printing) there is discoloration. It looks like gasolin spilled on the wet road (rainbow). Any idea and reason Ralf


brittle solder joint searches for Companies, Equipment, Machines, Suppliers & Information

Pillarhouse USA for Selective Soldering Needs

Training online, at your facility, or at one of our worldwide training centers"
Sell Used SMT & Test Equipment

High Throughput Reflow Oven
IPC Training & Certification - Blackfox

World's Best Reflow Oven Customizable for Unique Applications
Voidless Reflow Soldering

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...
Assembly Automation Technology

Original SMT Feeders and spares for Panasonic, Fuji , Yamaha, Juki , Samsung