Electronics Forum | Tue Feb 03 13:47:59 EST 2009 | grics
I would also suggest looking at your ramp rate in the cure oven. We noticed that accelerated heating increased the "gas out" of the solvent. We run 1A33 and and do not exceed a .5/degC ramp rate.
Electronics Forum | Wed Sep 02 11:36:22 EDT 2009 | kpm135
Is this an established process that is just now exhibiting these problems, or is this a brand new process you're just setting up? What is the rest of your process like? What is done to the boards before you coat them? Water washed? Solvent washed? Sa
Electronics Forum | Thu Jan 22 09:04:22 EST 2009 | mefloump
Humiseal recommends a 1 to 1 mix ratio of 1B31 and Thinner 521. I have for that I need to thin my ratio more to get humiseal to spray correctly in our PVA650. Also I am using Humiseal 1B73 but the tech data sheets say the same for spraying. Try thinn