Electronics Forum | Tue Oct 12 08:12:20 EDT 1999 | robert parker
any advice on smt resistors and capacitor that can survive an explosive shock. the ceramic smts are not, plastic ic's and discretes do fine.
Electronics Forum | Thu Feb 04 09:09:07 EST 1999 | dave
Can anyone help me with the pros and cons of trying to wave solder tantalum and large (1812) ceramic capacitors. I do know that one may see fractures on larger cermaic caps, but have not seen much on the tantalums. Any insight as to what problems I c
Electronics Forum | Fri Feb 05 09:39:58 EST 1999 | Dave F
| Can anyone help me with the pros and cons of trying to wave | solder tantalum and large (1812) ceramic capacitors. I do | know that one may see fractures on larger cermaic caps, but have not seen much on the tantalums. Any insight as to what proble
Electronics Forum | Tue Feb 16 16:28:30 EST 1999 | Tuffty
| | Can anyone help me with the pros and cons of trying to wave | | solder tantalum and large (1812) ceramic capacitors. I do | | know that one may see fractures on larger cermaic caps, but have not seen much on the tantalums. Any insight as to what
Electronics Forum | Thu Aug 17 23:44:26 EDT 2006 | guest
CBGA stands for Ceramic Ball grid array while PBGA stands for Ceramic Ball grid array. Noticable difference is the substrate used , one is using ceramic and one is using BT laminate. Regards
Electronics Forum | Fri Feb 16 11:07:25 EST 2007 | stepheniii
I'm not sure if anyone mentioned the single most important factor. p.m.'s. If the nozzles are getting dirty and clogged it's not going to do a great job of picking parts up. Don't think in terms of variation. It's there it's unavoidable and undet
Electronics Forum | Wed Aug 12 03:43:01 EDT 1998 | Terry Keen
We are taking enquiries for sub-contract work that we hope to be doing by Christmas. One of the enquiries is to assemble chip capacitors and an SO14 onto ceramic. Does the printing process, paste used and reflow process remain the same, or are there
Electronics Forum | Mon Jun 12 17:32:17 EDT 2006 | flipit
Hi, A little off subject but I just finished a quick little experiment where I placed 0201 to 1206 and some ceramic resonators at specific distances off the scored edge. The distances from scored edge ranged from 0.025" on up at 0.025" increments.
Electronics Forum | Mon Jan 19 09:07:45 EST 2015 | cotinc01
We can offer several nozzles to assist with the placement of 0402/0201 components in the four-spindle head. We offer the 06MPF along with custom ceramic tipped nozzles. Most of our standard nozzles for this head type are less than $125.00 each. Chec
Electronics Forum | Wed Aug 12 07:31:37 EDT 1998 | Earl Moon
| We are taking enquiries for sub-contract work that we hope to be doing by Christmas. One of the enquiries is to assemble chip capacitors and an SO14 onto ceramic. Does the printing process, paste used and reflow process remain the same, or are ther