Electronics Forum: certificate of analysis (Page 1 of 7)

Cost of labeling PCB's

Electronics Forum | Wed May 17 16:02:53 EDT 2000 | Mark J. Braska

Is there any data on the total cost of labeling PC boards. Included in this cost would be the labels, ribbons,printers & maintenance,software, and engineering & operator expenses(fully burdened). I am searching for an independant analysis of the co

Germanium doping of SN100

Electronics Forum | Mon Dec 17 12:15:10 EST 2007 | Claude_Couture

What a coincidence! Our last solder analysis showed our Ge to be .001% and the lab recommended to bring it up to .005% to get a better wetting. They even supplied a formula to calculate the amount to add based on the % and the quantity of solder in t

Visual Inspection of PCBA

Electronics Forum | Mon Oct 14 03:36:53 EDT 2019 | robl

Any major & stable new advances in the PCBA inspection arena anyone has seen recently? Marantz were looking into AI for simpler programming & defect analysis, and I saw some papers last year on neural networks & deep learning regarding inspection i

Shelf life of PCBs

Electronics Forum | Sun Mar 23 00:09:02 EST 2003 | MA/NY DDave

Know the specs your assembly is supposed to meet 2>Runs some lot soldering samples to minimize cost if you do decide to scrap or bake or ?? 3>Do at least a little post soldering analysis to assure yourself that the results are similar to experien

Water Absorption of PCB

Electronics Forum | Wed Feb 21 08:06:23 EST 2007 | davef

The cause could be a lot of different things. As long as you didn't use excessive reflow temperatures, we'd guess that: * Solder mask blister: Your board fabricator should be able to demonstrate through TMA [or equivalent] analysis that the mask wa

Design of Experiments

Electronics Forum | Fri Jun 26 08:58:43 EDT 1998 | Justin Medernach

| WHAT IS THE BEST ANGLE FOR THE SQUEEGEE BLADE TO BE ANGLED AT? WE ARE USING 45 DEGREE ON OUR POLYURETHANE BLADES, AND I BELIVE WE HAVE THE OPTION OF EITHER 45 OR 60 DEGREES ON OUR METAL BLADES. WHICH OF THE TWO IS BETTER, OR SHOULD WE BE USING AN

Re: Design of Experiments

Electronics Forum | Sat Jun 27 08:23:02 EDT 1998 | Dave F

| | WHAT IS THE BEST ANGLE FOR THE SQUEEGEE BLADE TO BE ANGLED AT? WE ARE USING 45 DEGREE ON OUR POLYURETHANE BLADES, AND I BELIVE WE HAVE THE OPTION OF EITHER 45 OR 60 DEGREES ON OUR METAL BLADES. WHICH OF THE TWO IS BETTER, OR SHOULD WE BE USING

Re: Design of Experiments

Electronics Forum | Tue Jun 30 11:12:19 EDT 1998 | Justin Medernach

| | | WHAT IS THE BEST ANGLE FOR THE SQUEEGEE BLADE TO BE ANGLED AT? WE ARE USING 45 DEGREE ON OUR POLYURETHANE BLADES, AND I BELIVE WE HAVE THE OPTION OF EITHER 45 OR 60 DEGREES ON OUR METAL BLADES. WHICH OF THE TWO IS BETTER, OR SHOULD WE BE USIN

PCB Manufacturers Certificate of Conformance

Electronics Forum | Wed Jan 02 04:05:46 EST 2002 | ianchan

Well usually QA keeps the COC and x-section samples, for a designated minimum time period of 6 months, this time period is not set in stone and is defined by your ISO records retention period...each company bears varient importance to the retention o

PCB Manufacturers Certificate of Conformance

Electronics Forum | Wed Jan 02 01:30:38 EST 2002 | Dreamsniper

Hi Guys, What most of you do with the above cert. of conformance that comes on a certain batch of PCB's from the PCB manufacturers ? It also comes with a micro section of a PCB showing the internal of a PTH Via Barrels. I kept receiving them from ev

  1 2 3 4 5 6 7 Next

certificate of analysis searches for Companies, Equipment, Machines, Suppliers & Information

Formic Reflow Soldering

Best Reflow Oven
Solder Paste Dispensing

We offer SMT Nozzles, feeders and spare parts globally. Find out more
High Throughput Reflow Oven

High Precision Fluid Dispensers
Sell Your Used SMT & Test Equipment

Wave Soldering 101 Training Course
design with ease with Win Source obselete parts and supplies

"回流焊炉"