Electronics Forum: chloride on pcb (Page 1 of 71)

solder balls on pcb

Electronics Forum | Thu Oct 23 23:38:48 EDT 2008 | pathakvj

We have 8 layer HASL PCB. We saw molten solder blobs / balls on op side of assembled PCB. (to check, if this was a bare board problem), We passed bare board as received thru, SMT reflow oven and saw solder balls on top side of board. What could be th

solder balls on pcb

Electronics Forum | Mon Oct 27 14:15:47 EDT 2008 | hussman

So you passed a BARE board thru the oven and got solder balls?

solder balls on pcb

Electronics Forum | Mon Oct 27 14:28:19 EDT 2008 | patrickbruneel

Do you refer to the highlight in the picture as a solderball? Looks more like copper to me.

solder balls on pcb

Electronics Forum | Thu Oct 30 19:59:05 EDT 2008 | gregoryyork

solder ball was caused by hasl process not reflow. seen before many times, look around wells of smt on bare boards should be more of them

solder balls on pcb

Electronics Forum | Fri Oct 24 06:55:48 EDT 2008 | clampron

Good Morning WS, If you experieced the solder balls after reflow of a bare board through the oven, then the source of the solder is either the oven or the board. I have had boards with untented via's that were HASL'd that had entrapped solder and fl

solder balls on pcb

Electronics Forum | Tue Nov 04 12:58:17 EST 2008 | smt123

I have to agree with Patrick here. This image appears to show a board that is NOT HASL as there is what appears to be a copper pad in the upper portion of the image. But then again the arrow tip appears to be white and I woudl expect that to be red s

raw copper on pcb

Electronics Forum | Thu Jun 07 05:11:42 EDT 2012 | cp38260

Hi, I have pcbs (Duroid/RT 5880) with raw copper, soldered in vapour-phase chamber at 230 degrees Celsius. During soldering, copper gets tarnished. Cleaning with Vigon A250 removes the tarnished layer. Indeed, in the VigonA250 techn. datasheet it is

ce mark logo on pcb ?

Electronics Forum | Wed Jun 11 04:10:26 EDT 2008 | bahabaha

Hi,, I need to put CE maek on my pcb , but I was told to follow the standard , what is the font type we need ? how can I add picture to pcb ?

ce mark logo on pcb ?

Electronics Forum | Wed Jun 11 07:44:04 EDT 2008 | davef

To get started, look here: http://en.wikipedia.org/wiki/CE_mark

how to control warpage on panelized pcb during reflow process

Electronics Forum | Thu May 23 10:21:19 EDT 2019 | emeto

What is the material of this PCB?

  1 2 3 4 5 6 7 8 9 10 Next

chloride on pcb searches for Companies, Equipment, Machines, Suppliers & Information

Precision PCB Services, Inc
Precision PCB Services, Inc

Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.

Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider

1750 Mitchell Ave.
Oroville, CA USA

Phone: (888) 406-2830