Electronics Forum | Mon Feb 23 20:27:31 EST 2004 | greg york
Is this a white residue on the joint and surrounding area's, if so the only thing I can remove it with after cleaning is an Isopar(Isoparrafinic hydrocarbon), my guess looking at other pastes where I have seen this is it is a type of wax used in form
Electronics Forum | Mon Feb 23 20:27:34 EST 2004 | greg york
Is this a white residue on the joint and surrounding area's, if so the only thing I can remove it with after cleaning is an Isopar(Isoparrafinic hydrocarbon), my guess looking at other pastes where I have seen this is it is a type of wax used in form
Electronics Forum | Tue Oct 31 21:49:38 EST 2006 | davef
First, we assume the white residue is only on the connector and not on other components. That would imply that either: * White stuff was on the connector when it came in-house from your supplier. [Confirm this theory by baking some connectors from
Electronics Forum | Sat Oct 29 20:29:30 EDT 2016 | adamjs
Posting here because all the threads asking for feedback on it are locked. We have been extremely happy with the 4300 tacky flux for BGA attachment. Not only is it both washable and no-clean (i.e. wash-optional), it was also the only tacky flux tha
Electronics Forum | Tue Dec 19 10:08:10 EST 2006 | George
Grant, Why don't you try a water-base flux which is No-clean, VOC-free also? I have tried the 270WR flux from AIM with good results even on lead-free process. My $0.02, George
Electronics Forum | Fri Mar 22 14:19:38 EDT 2019 | gregcr
Thank you ProcEng1 Nordson sent me a flux suggestion list: No Clean: 1. Kester Select 10 2. ALPHA EF-2210 3. AIM FX-16 Water Sol: KESTER 2331-ZX Nozzle Tinning: SUPERIOR #75
Electronics Forum | Mon Mar 29 09:33:37 EST 1999 | Chrys Shea
| I require some feed back from any one who knows about using a voc free flux in a nitrogen wave solder machine soldering both through hle and smt componants. | What disadvantages are there when using this flux? | Do you have any contact details with
Electronics Forum | Tue Mar 30 08:11:27 EST 1999 | George Steele
| | I require some feed back from any one who knows about using a voc free flux in a nitrogen wave solder machine soldering both through hle and smt componants. | | What disadvantages are there when using this flux? | | Do you have any contact detail
Electronics Forum | Wed Apr 27 08:19:41 EDT 2011 | charliedci
We are in the process of changing over our wave solder flux from alcohol based no clean to VOC free water based no clean. We are running an old Eletrovert with foam fluxer, tin lead solder. After preliminary testing on scrap boards and now starting t
Electronics Forum | Fri Mar 26 11:13:04 EST 2004 | Mike Konrad
jdomont, No-cleans are more difficult to clean than RMA�s. Even though no-cleans have a lower solids content than RMA�s, reflow and soldering profiles are normally more severe than those used for RMA. It is interesting to note that our most of our