Electronics Forum | Mon Aug 27 04:13:49 EDT 2012 | thmeier
Moisture should not be an issue with ceramics, but mechanical or thermal stress definitely is. Has there been rework on this capacitors? So check for handling /temperature of your soldering irons (better:use hot air). Check oven temperature/profile
Electronics Forum | Fri Jul 06 03:23:01 EDT 2001 | kennyhktan
Hi there Steven ! Please allow me to share some of my problem we're facing here with you. Here are a few points that I suggest you should check on your current process:- (1)PCB - Component land partern design ? It is per IPC spec ? - Mask
Electronics Forum | Wed Jan 07 07:16:25 EST 2004 | davef
Cold solder prior to properly performing a well designed drop test. Actually, "cold solder" means different things to different people. Two dull solder connection conditions are: * "Disturbed" solder joint: a solder joint that has an "angular face
Electronics Forum | Tue Jan 06 19:53:32 EST 2004 | jj
Hi, Any idea what's the possible causes of cold solder after drop test? Thanks JJ
Electronics Forum | Mon Feb 12 10:02:18 EST 2007 | rgduval
A little late to the party here, sorry... Has the joint been verified as a cold solder joint? That is, visually confirmed that it looks like cold solder, and, perhaps, xrayed to confirm the solder status? X-raying may sound a bit extreme, but you'
Electronics Forum | Mon Jan 19 14:54:38 EST 2004 | cyber_wolf
How did you come to the conclusion that you are having a cold joint problem. Just by appearance ? As Dave stated if you have any of the metals that he listed in the joints they will appear to be dull and grainy sometimes. But... Dave, I will have t
Electronics Forum | Tue May 30 13:50:40 EDT 2006 | Dragan
Hi, I ran into a problem and need a solution. It is a 3cm*4cm*1mm 2 layer PCB (6x6 panel) with a LQFP128 package Microcontroller, a resonator and 2 capacitors. What happens is: When i recieve the assembled pcbs from the assembly plant they wor
Electronics Forum | Tue May 30 17:17:08 EDT 2006 | Dragan
Hi, I ran into a problem and need a solution. It is a 3cm*4cm*1mm 2 layer PCB (6x6 panel) with a LQFP128 package Microcontroller, a resonator and 2 capacitors. What happens is: When i recieve the assembled pcbs from the assembly plant they wor
Electronics Forum | Tue Aug 25 20:33:31 EDT 1998 | Karlin
| | | | Hi, | | | | Does anyone has experiences in reflowing Ceramic BGA and found solder wicking ? Solder wicking has the syndrome that solder being wick from the pad and ended up in the leads. | | | | We have rule out the possibility of not printin
Electronics Forum | Thu Oct 27 00:45:41 EDT 2005 | pavel_murtishev
Good morning, I can recommend to use solder paste softeners, which can prepare solder paste for printing process. Softeners rise paste temperature by means of pseudo-planetary motion. Therefore, solder paste reaches room temperature during only 15