Electronics Forum | Mon May 22 10:41:50 EDT 2000 | Scott G
Can anybody provide information on shear testing of passive components. What standards are used etc. Thanks
Electronics Forum | Tue May 23 20:39:37 EDT 2000 | Dave F
Scott: Sounds like fun: � Solder joint strength in pull/shear varies with lead geometry, solder volume, lead metal/metallization, and the test method. � Among things, IPC-TM-650 talks to getting pads off-of boards. For instance: Method 2.4.8 is for
Electronics Forum | Wed Jul 03 15:40:17 EDT 2013 | davef
Shear tests are [in my opinion] senseless. The shear stress you measure depends more on the shear rate and on the point where the force is applied than on the grain structure. When shearing a component, you not only apply shear stress, but also roll
Electronics Forum | Fri May 17 16:53:50 EDT 2002 | davef
I recall a couple of papers in the SMTA 'Knowledgebase' that used ball shearing and an element in a study that compared BGA [maybe uBGA] component fabrication methods, er sumpin.
Electronics Forum | Fri Mar 30 20:06:55 EST 2001 | aortiz
Maybe there's no test and I don't know where or why my customer came with that requirement (I think because in one of the board shipments he got a board were a smd resistor broke, but I think that happened because miss handling), but anyway I need so
Electronics Forum | Fri Mar 30 13:06:50 EST 2001 | aortiz
Hi, I need support on the method or applicable standard to measure the shear force strength on chip capacitors and resistors. I know the soldered joints strength is related to land desing, solder volume, pcb and component solderability, component
Electronics Forum | Fri Aug 08 12:46:02 EDT 2003 | davef
When I was a salty old fart in the Navy, we sent the babes from the turnip patch off on snipe hunts. Shear tests are [in my opinion] senseless. The shear stress you measure depends more on the shear rate and on the point where the force is applied
Electronics Forum | Mon May 10 15:02:37 EDT 2004 | davef
There's no such specification. Not should there be. Shear tests [in our opinion] are senseless, because: * Solder joint strength in pull/shear varies with lead geometry, solder volume, lead metal/metallization, and the way the test is done. * She
Electronics Forum | Thu Nov 05 03:40:34 EST 2009 | valeo
Hi Rajeshmara, Mail sent with the datasheet of the glue we use in production. Thanks for first information you provide me for the shear specifications on 1206. But can you be more precise on this point ? How did you define it ? Is anyone have more
Electronics Forum | Wed Oct 06 22:55:14 EDT 2004 | davef
Your customer is correct. Components should not fall a board during a reasonable drop test. A shear test poorly represents a drop test. A drop test represents a drop test very well. If you want to proceed with shear testing, search the fine SMTne