Electronics Forum | Sat Feb 25 16:17:46 EST 2006 | A.N.other
Hi, been researching archives for PCB composition. Nothing much for what I want. Can anyone direct me/advise of PCB composition, and I mean the full works. Content of base materials, solder resist, chemical compositions of epoxy etc. Much appreciat
Electronics Forum | Thu Aug 24 16:44:27 EDT 2000 | Dr. Ning-Cheng Lee
There is no IMC composition can be identified in phase diagram of In/Sn. There are some compositions such as In3Sn or InSn4 cited in earlier literature. Those composition should be regarded as approximate representation of solid solution of In/Sn. I
Electronics Forum | Mon Nov 19 05:49:44 EST 2001 | Cheng
The BGA solder ball composition is 62/36/2 Sn/Pb/Ag, does any problem exist for the solder joint reliability? And what is the difference on SMTA process between this and the normal 63/37 ball?
Electronics Forum | Wed Dec 05 11:11:30 EST 2012 | eniac
SAC305 - it's just a metal composition of solder paste. All properties of solder paste depend on chemical composition of flux and other components - I don't know their names in English, sorry.
Electronics Forum | Thu May 18 21:05:58 EDT 2006 | Wizard of Oz Tin Man
"Solder alloy compositions are numerous but the most important are still the tin lead solders which were used by the Romans. Tin melts at around 232�C and lead at about 327�C in the combination 62Sn 38Pb the resulting alloy melts at 183�C. This compo
Electronics Forum | Fri Feb 09 02:30:50 EST 2007 | Muhammad Haris
What are Resins, Solvents, Activators, and Thickening Agents in Solder Paste and what are their helpful and harmful effects? AND What are the purposes/properties and effects of Sn(Tin), Pb(Lead), Ag(Silver), Bi(Bismuth), In(Indium), Cu(Copper), Ni(
Electronics Forum | Tue Aug 22 16:43:57 EDT 2000 | David Snyder
Hello Dr. Lee, Will no-clean fluxes be more of a challenge to develop?
Electronics Forum | Mon Sep 14 09:09:10 EDT 1998 | Earl Moon
| I am running composite fixtures on my wave solder machine and after about 500 passes each (1 month)they are showing serious signs of wear in that the composite surface is bubbling up and glass fibers are also starting to show. | The problem here
Electronics Forum | Mon Apr 22 21:10:07 EDT 2002 | davef
Russ: What is the composition of this non-ionic material on your pads?
Electronics Forum | Thu May 01 16:36:49 EDT 2003 | blnorman
What is the best way to determine solder joint intermetallic composition? Metallography? XDS of the joint? Any input is appreciated.