Electronics Forum | Mon Apr 04 08:45:42 EDT 2005 | jimih280
how does polyurethane used for wood floor coating differ from urethane conformal coatings sold for circuit boards? where can i get uv tracer to put in oil based urethane?
Electronics Forum | Wed Feb 23 22:38:28 EST 2005 | davef
We: * Cure 1B73 according to spec in a heat box, like a Blue-M * Clean nozzles [one set in use, one set being cleaned] in thinner in a bronson ultrasonic cleaner * Haven't evaluated coatings in years, but would do it according to J-STD-001C, Reqmnts
Electronics Forum | Thu Feb 17 15:01:23 EST 2005 | davef
We're not familiar with your DYMAX #984-LVUF. The problem is not with your conformal coating. The problem is with your 0805 [and not all of 0805, probably just those from a specific supplier]. This lack of coverage of components is called dewetting
Electronics Forum | Thu Mar 08 01:19:16 EST 2001 | Mike Moninger
The environment essentially defines the need for coating. "Inside" may mean inside a men's locker room with attendant high humidity or inside a climate-controlled clean environment. Conformal coatings offer protection against moisture, fungus, chemi
Electronics Forum | Wed Oct 27 13:20:47 EDT 2004 | DavidB
We are producing boards with Alpha 591S RMA No-Clean paste and are coating after SMC with Dow silicone ( toluene solvent based) conformal coating. We have experienced several failures due to soft shorts ( electrochemical migration?) We have also obse
Electronics Forum | Wed Feb 23 10:01:00 EST 2005 | frankracine
Dave, Few questions concerning your Umiseal 1B73. To cure your Acrylic coating do you respect specification ( 2Hrs-170degree F) or you go faster than that? What do you use to cure it? Do you have to clean your nozzles each day or each monday beca
Electronics Forum | Sun Apr 10 03:25:35 EDT 2005 | Peter
Normally, some conformal coatings do not have very good wetting properties, that should be basic function of a good coating material (the same reqirement as avoid bubbles during coating process)! For UV curing conformal coatings, you can try Lackwe
Electronics Forum | Fri Sep 11 12:08:10 EDT 2015 | derrikf
I built one using an old Asymtek Automove. When all was said and done, it cost less than $400, including what was paid for the machine itself. It's a very basic setup, (air over syringe), but for our needs it does everything and more. With air to syr
Electronics Forum | Fri Nov 21 18:56:41 EST 2003 | jsloot
Gun wash is another term used for acrylic laquer thinner. We use DuPont 3642SC. We have much success in its use.
Electronics Forum | Mon Apr 08 14:16:29 EDT 2019 | sever_83
We've never heard of seen of such a thing either. We tried a clean sample board and applied con coat. Same process through out and we saw nothing. After speaking with the original operators who was curing the boards he had left the boards much longer