Electronics Forum: conformal coating use by (Page 1 of 50)

conformal coating

Electronics Forum | Fri Apr 17 14:08:00 EDT 2015 | davef

Humiseal says, "UV cure – These materials are also more difficult to repair as they are the most chemically resistant and mechanically tough of all conformal coatings. Removal is possible locally by using powder abrasion."

conformal coating

Electronics Forum | Mon Apr 04 08:45:42 EDT 2005 | jimih280

how does polyurethane used for wood floor coating differ from urethane conformal coatings sold for circuit boards? where can i get uv tracer to put in oil based urethane?

conformal coating

Electronics Forum | Wed Jul 06 20:15:51 EDT 2005 | Gary Bremer

The good old days weren't all that bad. When I needed to have a specification callout for a conformal coating on an engineering drawing, I just used MIL-I-46058, type UR (for example), and the drawing checkers were quite happy. Since MIL-I-46058 ha

conformal coating

Electronics Forum | Thu Jul 07 06:48:15 EDT 2005 | davef

Alternatives are: * DSCC Columbus continues to maintain the QPL for MIL-I-46058C. [Engineering is unlikely to change.] * Use International Electrotechnical Commission Standard, IEC 61086 - Coatings for loaded printed wire boards (conformal coatings)

conformal coating

Electronics Forum | Wed Jul 06 22:34:19 EDT 2005 | davef

Many companies use IPC-CC-830B as a replacement for the deactivated MIL-I-46058 conformal coating standard.

conformal coating

Electronics Forum | Thu Jul 07 00:53:12 EDT 2005 | Gary Bremer

Curtiss-Wright uses MIL-I-46058 at present. Any suggestions on how to approach engineering and update the drawings for new contracts?

Is conformal coating necessary?

Electronics Forum | Tue Mar 06 17:14:40 EST 2001 | bschwyn

Is conformal coating necessary for products that are used indoors?

Problem with conformal coating

Electronics Forum | Thu Feb 17 10:33:53 EST 2005 | Frank R.

I use conformal coating DYMAX #984-LVUF and I don't know if it's a problem of viscosity but 0805 components are not covered properly. We use a dispensor to applied it and we cured it by UV. Even if I apply a thicker layer, the coating seems to have

PCB conformal coating

Electronics Forum | Fri Jul 04 06:29:51 EDT 2008 | andrzej

Hi, 1. we use John C. Dolph company - AC-46 on production line. I dont get any benefits advertising this on forum (but I`d wish to ;) 2. we use stickers, or other hand made tools to cover areas from AC-46 - it depednds on need for project.

AVR80 BA conformal coating

Electronics Forum | Wed Mar 04 10:23:03 EST 2015 | rgduval

I haven't used this particular CC, but...found this in their data sheet: "AVR 80 BA Conformal Coating will be touch dry after 15 - 20 minutes at room temperature and does not require a thermal cure. The full properties of the coating will be obtaine

  1 2 3 4 5 6 7 8 9 10 Next

conformal coating use by searches for Companies, Equipment, Machines, Suppliers & Information

SMT spare parts - Qinyi Electronics

Component Placement 101 Training Course
Global manufacturing solutions provider

Reflow Soldering 101 Training Course
2024 Eptac IPC Certification Training Schedule

Best Reflow Oven
thru hole soldering and selective soldering needs

Training online, at your facility, or at one of our worldwide training centers"
PCB Depanelizers

Low-cost, self-paced, online training on electronics manufacturing fundamentals