Electronics Forum | Mon Aug 27 10:09:50 EDT 2001 | gresko
Steve, Depending on the type of equipment you are using for P&P you may want to consider placing and processing the substrates in Auer boats. I have provided many applications for ceramic substarate users using purchased Auer boats or machined palle
Electronics Forum | Wed Aug 22 21:00:41 EDT 2001 | dlkearns1
Yes, it is very true and very clean SNAP!
Electronics Forum | Sat Aug 25 13:24:37 EDT 2001 | btaylor
We have used scribed ceramic from CoorsTek for many years with no problem. You will have to control your scribe depth so not to break it during processing. If you have any more question you can e-mail me.
Electronics Forum | Wed Aug 22 18:51:48 EDT 2001 | stefo
Hi ya'll, We may be getting some business here for a small (2" X 2"),ceramic substrated, double-sided SMT assembly. I've done ceramic substrates with SMT in the past, but not double-sided, and as packed as this thing will be... My question is, can
Electronics Forum | Wed Aug 22 21:11:25 EDT 2001 | davef
When it works right, it's a beautious thing. => When goes wrong, you have one board with some of the other board's material, not too coo. Scribed and broken ceramic has bad-butt sharp edges. You'll feel this sticky stuff on your hands, look down,
Electronics Forum | Sat Jun 19 00:49:17 EDT 2010 | mun4o
Hi all, lately ofen I have problem with cracked ceramic capacitors.We use 0805 and 0603 cap. Samsung.ICT measure diferent capacity of nominal.If I tray to desoldering component , then component cracked.I think , that the reason is the moisture in com
Electronics Forum | Sat Jun 19 08:32:49 EDT 2010 | davef
Please describe the location and appearance of the crack
Electronics Forum | Mon Jun 21 02:15:03 EDT 2010 | ppcbs
We also encountered the crack case in multi layer Ceramic Cap,0603 after touch up. Most failure were on the terminals. Previously, we used 0805 instead 0603.that time, failure were very few.
Electronics Forum | Fri Jun 25 05:34:40 EDT 2010 | ppcbs
Hi iv40 Try with NIC ceramic capacitor that was tested in wet process. We hav succeed with these cap after we found some failure with Kemet ceramic Cap which tested in dry test process while manufacturing.
Electronics Forum | Mon Jun 21 12:02:36 EDT 2010 | roland_grenier
check your de-panelling process if you are using break-out tabs or V scoring.