Electronics Forum | Tue Sep 04 18:11:18 EDT 2001 | davef
Assuming you're asking about double sided reflow soldering ... Use pad mating to lead wetting area. Bob Willis has found the ratio to be as much as 44 grams/sq in. Check Bob's site [Electronic Presentation Sevices] for more. Phil Zarro uses the
Electronics Forum | Sun Feb 25 17:22:05 EST 2001 | itm
Steve, Neil, John and everyone else - The ITM site is alive and well ! Regarding registration: we do not have an autobot to handle registration - we do it manually every few days. I have been on vacation for the past week (to a wonderful place whe
Electronics Forum | Sun Feb 25 17:22:09 EST 2001 | itm
Steve, Neil, John and everyone else - The ITM site is alive and well ! Regarding registration: we do not have an autobot to handle registration - we do it manually every few days. I have been on vacation for the past week (to a wonderful place whe
Electronics Forum | Thu Jan 12 13:58:13 EST 2006 | sarar
I agree. Phil is a very respectable guy who knows what he's talking about, and his writings are well-done. I'm sure there are some consultants out there who are less than par, and the profession as a whole has a stigma of just rambling a bunch of m
Electronics Forum | Mon May 10 08:00:14 EDT 1999 | Timothy O'Neill
| | | | I am about to embark on an effort to evaluate 3 different solder material suppliers and their recommended materials for our assembly process, in an effort to find the best supplier/material. We do mixed technology, with NOCLEAN chemistry so
1 |
Products, services, training & consulting for the assembly, rework & repair of electronic assemblies. BGA process experts. Manufacturers Rep, Distributor & Service Provider for Seamark/Zhuomao and Shuttle Star BGA Rework Stations.
Training Provider / Manufacturer's Representative / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
1750 Mitchell Ave.
Oroville, CA USA
Phone: (888) 406-2830