Electronics Forum | Mon Aug 12 15:56:13 EDT 2013 | pjchonis
Vapor phase soldering systems by Asscon are characterized by special designed heating modules. The thermal mass of the heating modules is designed so that a completely delay-less and direct regulation of the heat/flow/energy transfer to the soldering
Electronics Forum | Wed Nov 17 09:28:40 EST 1999 | Steve Z
Hello, I am new to the SMT area and I need to know what a "good" vapor phase reflow profile should look like. The fluids we are using have a BP of 45 C and 219 C. Thanks,
Electronics Forum | Wed Jul 10 14:29:27 EDT 2013 | isd_jwendell
You wouldn't have a very good profile if you went straight from room temp to vapor temp (_-). The chamber should preheat the board before using vapor to melt the solder.
Electronics Forum | Mon Jul 19 11:11:18 EDT 1999 | Wolfgang Busko
| Perhaps a little hard to find but is there anyone who uses a vapor phase process to solder populated card with BGAs. I am interested in the success rate of such a process. It is obvious that the throughput is reduce vs a convection oven but still t
Electronics Forum | Mon Jul 19 11:50:47 EDT 1999 | Mario
| | Hi, SMTASSY | | that�s what we do, soldering our double-sided-finepitch-BGA-and all-the-other-stuff-boards in vapourphase because it�s the only thing we have. | First, we do not do real series produktion, only prototyping up to sometimes 20 uni
Electronics Forum | Mon Jul 19 12:37:15 EDT 1999 | Wolfgang Busko
| | | | | Hi, SMTASSY | | | | that�s what we do, soldering our double-sided-finepitch-BGA-and all-the-other-stuff-boards in vapourphase because it�s the only thing we have. | | First, we do not do real series produktion, only prototyping up to som
Electronics Forum | Tue Jul 20 05:29:14 EDT 1999 | Wolfgang Busko
| | | | | | | | Hi, SMTASSY | | | | | | that�s what we do, soldering our double-sided-finepitch-BGA-and all-the-other-stuff-boards in vapourphase because it�s the only thing we have. | | | First, we do not do real series produktion, only prototypi
Electronics Forum | Wed Mar 12 15:26:46 EDT 2014 | dan_ems
Hello, in my SMT process I have some problems with the solderability (look like dewetting) on a PCB with finish HASL Lead Free with a composition that is melt at 230 degree Celsius. My oven is with vapor phase and the peak temperature is 230 degre
Electronics Forum | Mon Aug 16 20:19:10 EDT 2004 | Grant
Hi, We have both Vapor Phase ASSCON semi auto as well as Soltec convection inline ovens. I must say we had no end of problems with Vapor Phase. We tried everything, and just could not totally eliminate tomb-stoning completely. We would always get a
Electronics Forum | Tue Aug 18 10:11:04 EDT 2009 | grantp
Hi, Yes, I think this sounds like a form of tomb-stoning, and we used vapor phase until it ended up driving us totally nuts trying to deal with tomb-stoning. We tried everything, and all kinds of stencil apertures. Vapor phase is an amazing process
Main Products: 1. Original new and Original Used SMT/AI Spare Parts. 2. SMT Equipments And Related Machine( SMT Calibration, SMT Feeder Carts,Conveyer etc.) 3. Maintenace and Repair Service Pre-Sales Service Provide details ab
Manufacturer's Representative / Manufacturer / Equipment Dealer / Broker / Auctions / Consultant / Service Provider
Building A, Jiepeng Square, Fuyong
Shenzhen, 30 China