Re: haloing on SMT PCBs

Electronics Forum | Mon Jun 08 15:01:02 EDT 1998 | D.Lange

| I work QA at an OEM in Alberta, Canada. I saw earlier posts on the smtnet regarding PCB haloing criteria. I am currently in a dispute with my PCB vendor over the acceptability of haloing (delamination) around plated through holes and vias on a lot

Depanel thin board

Electronics Forum | Fri May 29 07:17:30 EDT 2015 | kkay

We have a small board about 1" by .5" and it is .012" thick. It is in a 50 up panel. We have tried rat bites and v-score and we keep seeing delamination around the edges. Anyone have experience depaneling boards this thin?

Repair of FR4 double-sided pcb

Electronics Forum | Thu Aug 22 07:48:30 EDT 2002 | Dave Milk

While separating individual pcbs from a panel, operators have caused delamination of the edge of the board, at the tabs that were cut. How can these boards be repaired? The delamination causes them to fail J-STD-001C 9.2.1.1.d. Also, what would yo

Mechanical Delamination at de-panel

Electronics Forum | Mon Jun 02 15:03:05 EDT 2014 | clydestrum

Background on the PCB: Thickness: .032" Material: Standard Fr4 V-score: Leaves .016" (approx .008" cuts on either side) We are having some issues on these boards where the edges are delaminating all the way to the copper during de-panel. Now, we are

BGA short

Electronics Forum | Thu Dec 15 09:05:44 EST 2005 | russ

These random shorts, are they most prevailent on the edges, corners, or truly all over the place. It almost sounds like package warp/delamination or something of that nature. Are you baking parts per MSL requirements?

Re: PCB panellisation

Electronics Forum | Sun Apr 05 14:57:10 EDT 1998 | Earl Moon

| | | | | We are in the process of deciding whether to change a PCB product from a single board to a 3 up panel array. Could you please advise on the most effective removal design, either scoring or snap off, taking into account that material utili

Re: depaneling machines

Electronics Forum | Thu Dec 23 15:10:50 EST 1999 | Victor Salazar

What we did was design or panels with routed out edges held on by tabs. This was very effective. All we use is a pair of pneumatic scissors to cut off the tabs. We are using from single-to 13 layer PCB's and we have had no problems with delamination

Damaged PCB.. what do you think?

Electronics Forum | Fri Mar 16 10:04:41 EDT 2012 | davef

We'd repair a drop board like this. Here's what our old friend Jeff Ferry said is a published article ... When boards lose their edge: when the corner of a circuit board breaks or is damaged, the problem cannot be ignored by Jeff Ferry One of the m

Questions About Risk of PCB Delamination as a Result of Moisture Build Up After Damage to Solder Mask

Electronics Forum | Tue Apr 23 10:31:59 EDT 2019 | laserpro

Hi all and thanks for viewing my post! My questions related to the subject line are as follows: 1. Does the Epoxy Solder Mask Layer of a PCB protect against moisture absorption? Is this a primary function of the solder mask? 2. Does exposed FR4 na

baking boards, revisited

Electronics Forum | Fri Oct 04 11:34:42 EDT 2002 | Bob Willis

Some additional comments from a paper may be of interest. Baking Printed Circuit Boards - Why and How Baking printed boards prior to conventional and surface mount assembly should not be necessary. Often boards are baked for historical reasons; in

  1 2 Next

edge delamination searches for Companies, Equipment, Machines, Suppliers & Information

Selective Soldering Nozzles

Training online, at your facility, or at one of our worldwide training centers"
SMT feeders

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...
Shenzhen Honreal for all your SMT Equipment needs

Easily dispense fine pitch components with ±25µm positioning accuracy.
2024 Eptac IPC Certification Training Schedule

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.


"Heller Korea"