Electronics Forum | Wed Jun 25 09:51:51 EDT 2014 | iam09
Hi Sirs, We are running Tin Lead process and we have boards that required clean and no clean process which have different flux application in our wave process. We are looking into opportunity to use common flux system for both clean and no clean an
Electronics Forum | Thu Aug 09 16:41:12 EDT 2001 | johnw
Dave , you know it's your cheery disposoition I love.... Ok so the process: Process is Double sided reflow for SMT & PTH via the wave. Like I said or did I, I forget and can't check back...it's a spray fluxer with noclean mutlicore NR3s-06 water b