Electronics Forum | Thu Jun 09 21:45:23 EDT 2005 | davef
We don't know, but we'd contact Enthone-OMI [ http://www.enthone-omi.com ] for suggestions. Enthone makes materials used by fabricators of HDI, microvia boards.
Electronics Forum | Thu Sep 15 19:58:35 EDT 2005 | davef
Shikoku Glicoat SMD process is the market share leader for LF OSP in Japan and the Asian Rim. Enthone Entek is more of a US / Euroland product. Beyond that, it's not clear that Enthone has kept pace with product development necessary to compete in L
Electronics Forum | Thu Jan 22 08:48:42 EST 2004 | patrickbruneel
Kris, You will need to change your probes to "bite" into the surface twisting probes specialy designed for copper surfaces. The surface hardness of copper is a lot higher compared to tin. link to article from osp manufacturer (see page 5) http://www
Electronics Forum | Tue Sep 26 20:19:51 EDT 2000 | Dave F
Never heard of N-Tech. Whose material do they use? Two common materials are: Imidazole (Via Systems) and Entek (Enthone) OSP is a lacquer that fabs apply to boards by either spraying or dipping. What thickness control does your fab use? For inst
Electronics Forum | Mon Jul 03 17:12:49 EDT 2000 | Ramon I Garcia C
Hi!!! I think, you should visit www.enthone.com this it's the internet place of an inks company named Polyclad Technologies. I hope this information can help you...
Electronics Forum | Wed Feb 28 10:00:46 EST 2001 | dason_c
Please advise what kind of the solder mask, glossy or matt? Matt finished can reduce the solder ball significant. Check Enthone, Enplate DSR Series. Good Luck!
Electronics Forum | Mon May 13 14:15:46 EDT 2002 | davef
Entek is Enthone's OSP [organic solderability protection]. It is widely used in the PCB fabrication business. Imidazole (Via Systems) is good, but is not as widely available. Search the fine SMTnet Archive on: * OSP * Entek CU-56, Entek Plus CU-10
Electronics Forum | Mon Sep 29 11:57:10 EDT 2008 | davef
These streaks could roller marks. Look here [ http://www.enthone.com/docs/AlphaSTAR-UP2-Troubleshooting.pdf ] near the bottom of page 1.
Electronics Forum | Thu Jun 14 21:14:04 EDT 2001 | davef
There�s tons of stuff on-line. Do a net search on "immersion silver". Examples are: * http://www.smta.org/knowledge/proceedings_abstract.cfm?PROCEEDING_ID=571 * http://www.enthone-omi.com/articles/FinalFinishesT1.pdf * http://www.epa.gov/opptintr
Electronics Forum | Thu Sep 14 20:11:19 EDT 2006 | davef
You weren't specific about the OSP that you use. We use Entek Plus CU-106A. Yes, just about everything removes Entek, especially if there's heat involved. Ethone states: * Alcohol strips 70% of the coating * Water removes 15% * Kyzen Lonox only t