Electronics Forum: example of date codes (Page 1 of 1)

Shelf Life of Components (solderability)

Electronics Forum | Tue Feb 15 21:27:18 EST 2005 | davef

Component shelf life depends on: * Solderability protection type. * Quality of process and materials used in applying solderability protection. * Duration of time from when the solderability protection was applied. * Packaging used in component stor

Solderability of Resistor Network Arrays

Electronics Forum | Thu May 30 11:37:27 EDT 2002 | Ron Costa

Hi Ray, A couple of things to look into: 1.date code of reel 2. what is the termination made up of tin/lead or tin/lead/palladium. Check with part manufacturer. 3.paste volume/aperture openings 4.PCB plating 5.solder paste formulation Good luck R

Re: Shelf Life of Components

Electronics Forum | Fri Dec 03 18:01:39 EST 1999 | Dave F

Chris, Two points of perspective are: 1 Solderability: The shelf life of components has elapsed when they are no longer solderable. There's tons of variables that affect this, but keys are: * Intermetalics grow as a function of temperature. * Th

Re: Serial Numbering of PCB's (?)

Electronics Forum | Thu Feb 03 11:20:15 EST 2000 | John O'Brien

This is getting to be a more common practice, especially with the application of a 2-D bar code directly to the board (via laser, ink jet,etc.) Some really major companies are jumping on the bandwagon because it also allows treating each board as a l

Re: Bow and Twist of PCB's

Electronics Forum | Wed Aug 19 08:00:55 EDT 1998 | Earl Moon

| Hi there, | I'm actually facing a lot of trouble with PCB's presenting up to 3mm of bow /twist at reception i.e. before assembly. The PCB size is 220 by 230mm. The boards are to be assembeled SMD double sides with 05.mm pitch on both sides. In orde

Part of PCB silkscreen turns yellow brownish

Electronics Forum | Fri Aug 29 09:39:08 EDT 2014 | rgduval

I'll try to deal with the issues as you've presented them. 1. Blistering/delamination, shown in photo 2. The most likely cause of blistering/delamination like this is moisture in the boards. The moisture can get into the boards in multiple ways..

Re: QFP On both side of a board

Electronics Forum | Fri Dec 11 16:06:18 EST 1998 | Michael Allen

G, You'll find at least one old thread in this Forum on dual-reflow if you do a search. I found one dated April 7, '98 (searched on "reflow"); this particular thread includes a discussion about the maximum weight-to-surface_area for successful dual

Re: Marking Codes

Electronics Forum | Tue Jan 05 14:37:18 EST 1999 | Dave f

| I would like to know if it exist a croos reference book for marking code on smt device? | I'm fixing a unit now and try to know what are the following devices: | The look like transistors and are mark like that "8A" |

  1  

example of date codes searches for Companies, Equipment, Machines, Suppliers & Information

pressure curing ovens

Training online, at your facility, or at one of our worldwide training centers"
convection smt reflow ovens

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...
2024 Eptac IPC Certification Training Schedule

Have you found a solution to REDUCE DISPENSE REWORK? Your answer is here.
PCB Handling Machine with CE

Software for SMT placement & AOI - Free Download.
Electronics Equipment Consignment

High Precision Fluid Dispensers