Electronics Forum | Wed Jul 01 13:57:07 EDT 2015 | circleprime
I have a customer that is requesting their flex circuit be conformally coated. Is this something that is done? Which coating would stand up to the stresses of flexing? Wouldn't that put stress on the components? Thanks! Shannon
Electronics Forum | Tue Sep 08 16:32:23 EDT 2015 | duso02
Commonly done with Parylene.
Electronics Forum | Wed Jul 29 11:28:54 EDT 2015 | pankyb1261
How many times does it have to flex. There are acrylic conformal coatings that can be bent once to 90 degrees or so
Electronics Forum | Fri Jul 24 16:39:16 EDT 2015 | cnotebaert
have done it in the past, used silicon as it will flex,, however its not the most robust material! tends to peel/flake off.
Electronics Forum | Mon Oct 14 15:13:52 EDT 2013 | esoderberg
Does anyone have a novel idea on how to protect the flex area during conformal spray coating? Currently using Humiseal T30 on the flex but it has to be removed very carefully to insure coating stays intact on the board.
Electronics Forum | Mon Apr 04 08:45:42 EDT 2005 | jimih280
how does polyurethane used for wood floor coating differ from urethane conformal coatings sold for circuit boards? where can i get uv tracer to put in oil based urethane?
Electronics Forum | Thu May 20 14:32:06 EDT 2010 | davef
First, what's wrong with some dewetting of conformal coating on component bodies? Second, there are chemistries that might be able to remove silicone mold release, but cleaning the chemistry is not easy without affecting the whole board, as you impl
Electronics Forum | Fri May 26 04:58:19 EDT 2023 | auriga2001
I agree with the two other replies. Left alone, it is a defect. If it's just excess adhesive or coating, you can use IPC-7711/7721 'Rework, Modification and Repair of Electronic Assemblies' for guidance on removing. Section 2.3.1 explains how to te
Electronics Forum | Tue Jan 13 16:40:03 EST 2004 | Jacob Lacourse
Hi folks, I have a conformal coating application where I need the coating to be UV stable for a number of years without any crazing or cracking of the coating. I have looked for such a coating and have come up empty handed. Much of the circuit boar
Electronics Forum | Thu Jun 27 08:47:21 EDT 2019 | SMTA-John
Having success with Circuit Boards #432 Solvent Resistant Ink - Designed specifically for circuit boards. This medium dry ink is highly resistant to solvents .... It is also non-conducting. Note: this ink contains an aggressive solvent so should not
Midwest Circuit Technology provides Carbide Router Bits and End Milling Cuters for use in PCB Depaneling equipment. We have over 35 years of supplying tools and machining experience in drilling, Routing, Test Fixture manufacture.
114 Barrington Town Square
Aurora, OH USA
Phone: 13309956900