Electronics Forum | Wed Dec 22 18:09:07 EST 2004 | kmorris
At a previous job I had been taught that when reflow soldering polyimide flex circuits, it was necessary to pre-bake them before reflow soldering to prevent delamination. Our procedures said that there must be a 1hr bake prior to reflow, and the flex
Electronics Forum | Wed Dec 22 21:14:53 EST 2004 | davef
IPC-FA-251 recommends 121*C for 30-60 minutes for 1 and 2 flex layer circuits. A rigid flex can take easily an hour per layer depending on the construction.
Electronics Forum | Fri Jul 24 16:39:16 EDT 2015 | cnotebaert
have done it in the past, used silicon as it will flex,, however its not the most robust material! tends to peel/flake off.
Electronics Forum | Wed Jul 29 11:28:54 EDT 2015 | pankyb1261
How many times does it have to flex. There are acrylic conformal coatings that can be bent once to 90 degrees or so
Electronics Forum | Tue Mar 21 19:34:32 EST 2006 | Tom Smykowski
Omar: I dealt with this so called "hot bar" process also, and you're right; it's neither reliable nor repeatable. The goal was to attach a flex LCD display to another flex circuit. The flex LCD was constructed of resin and conductive silver particl
Electronics Forum | Sat Jan 21 13:49:14 EST 2023 | pcbsino
perhaps we can help you for this SMT and THT part soldering problem, better not bend it not too hard. Electronic manufacturing pcbsino.com
Electronics Forum | Wed Dec 22 23:29:57 EST 2004 | KEN
Check with Dupont's web site. They have a wealth of information on the various polyimide products they manufacture. I was quite surrised at the differences in materials and in particular the dimensional stability and hydroscopy. Good stuff mayna
Electronics Forum | Mon May 27 18:25:03 EDT 2002 | Carol Stirling
Thanks for the information Reworkman, We are leaning to the theory of better safe than sorry. I think I'd supply the bags and dessicant just to eliminate manufacturing issues. What temps & times do you ask your boardhouse to bake to? Ours said some
Electronics Forum | Wed May 08 11:07:54 EDT 2002 | Carol Stirling
We have a concern with moisture absorbtion/humidity effects on PWBs specifically used for automated SMT (including BGA). I'm sure there is a IPC spec on this and would appreciate the number - I've searched the IPC web-site -no results. Could you t
Electronics Forum | Tue May 21 17:25:28 EDT 2002 | Carol Stirling
Hi Dave F, Thanks for the reply, the question was Customer driven. Could you clarify your recommendations for heat sealed moisture barrier bags please - does this include Nitrogen vac pack? Our production runs are small, so there is an investigat
Midwest Circuit Technology provides Carbide Router Bits and End Milling Cuters for use in PCB Depaneling equipment. We have over 35 years of supplying tools and machining experience in drilling, Routing, Test Fixture manufacture.
114 Barrington Town Square
Aurora, OH USA
Phone: 13309956900