Electronics Forum | Wed Jul 01 13:57:07 EDT 2015 | circleprime
I have a customer that is requesting their flex circuit be conformally coated. Is this something that is done? Which coating would stand up to the stresses of flexing? Wouldn't that put stress on the components? Thanks! Shannon
Electronics Forum | Tue Sep 08 16:32:23 EDT 2015 | duso02
Commonly done with Parylene.
Electronics Forum | Wed Jul 29 11:28:54 EDT 2015 | pankyb1261
How many times does it have to flex. There are acrylic conformal coatings that can be bent once to 90 degrees or so
Electronics Forum | Fri Jul 24 16:39:16 EDT 2015 | cnotebaert
have done it in the past, used silicon as it will flex,, however its not the most robust material! tends to peel/flake off.
Electronics Forum | Mon Oct 14 15:13:52 EDT 2013 | esoderberg
Does anyone have a novel idea on how to protect the flex area during conformal spray coating? Currently using Humiseal T30 on the flex but it has to be removed very carefully to insure coating stays intact on the board.
Electronics Forum | Mon Apr 04 08:45:42 EDT 2005 | jimih280
how does polyurethane used for wood floor coating differ from urethane conformal coatings sold for circuit boards? where can i get uv tracer to put in oil based urethane?
Electronics Forum | Tue Jan 13 16:40:03 EST 2004 | Jacob Lacourse
Hi folks, I have a conformal coating application where I need the coating to be UV stable for a number of years without any crazing or cracking of the coating. I have looked for such a coating and have come up empty handed. Much of the circuit boar
Electronics Forum | Thu Jun 27 08:47:21 EDT 2019 | SMTA-John
Having success with Circuit Boards #432 Solvent Resistant Ink - Designed specifically for circuit boards. This medium dry ink is highly resistant to solvents .... It is also non-conducting. Note: this ink contains an aggressive solvent so should not
Electronics Forum | Tue Jun 02 18:01:47 EDT 1998 | Earl Moon
| | | We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is no
Electronics Forum | Tue Jun 02 14:32:58 EDT 1998 | Chris Fontaine
We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not alwa