Electronics Forum | Thu Jan 18 12:21:57 EST 2007 | tonang
How to reduce flux contain on PCB after reflow process?
Electronics Forum | Mon Mar 25 21:45:22 EDT 2024 | buckeye
I got an inquiry from one of our electronics labs with regards to their soldering processes. They use eutectic (63% Sn, 37% Pb) solder. For liquid flux they are currently using Kester 186, which is an old-school, full rosin (RMA and ROL1) flux that c
Electronics Forum | Sun Oct 11 00:23:26 EDT 1998 | MIKE
| Came a cross an interseting observation/question. | I'll need to filter additional information and specifics to those whom may be able to assist me. But for now; | | I use a water soluble base organic flux manufactured by Kester (the exact soluti
Electronics Forum | Mon Oct 12 20:51:14 EDT 1998 | Eric
| | Came a cross an interseting observation/question. | | I'll need to filter additional information and specifics to those whom may be able to assist me. But for now; | | | | I use a water soluble base organic flux manufactured by Kester (the exac
Electronics Forum | Mon Jan 07 21:07:00 EST 2002 | davef
Using a flux pen sounds like a good idea. Comments are: * I assume you�re talking aqueous flux. If not, some NC flux pens leave white residues. Nearly all of 15 samples suffered to varying degrees with white residues. * Use the same flux that you
Electronics Forum | Mon Feb 18 15:20:43 EST 2008 | kennyg
A PCBA contains a couple of parts that are not sealed and can't be water washed. We hand solder these with no-clean after everything else is water washed. The designer says the no-clean residue must be completely removed so that it will not affect
Electronics Forum | Tue Dec 26 10:54:37 EST 2006 | yusufgomec
We use hot air leveling (HAL) process in pcb production. HAL process is 3 steps. �n 1. step flux. 2. step is HAL. And 3. step is rinsing. As you know there is mustn't any flux after rinsing operation. Our flux chemical is water soluable. But there ar
Electronics Forum | Thu Mar 02 11:20:25 EST 2017 | tombstonesmt
Our Senju Sparkle Flux contains 8% solids and is a NC.
Electronics Forum | Tue Sep 21 13:10:10 EDT 1999 | Dave F
| Dear All, | | In order to understand the soldering technologies in SMT, I'd like to understand why some cards are soldered and then cleaned, or only soldered whitout water cleaning nor "ultra sound" wavelength. | | I mean that I wonder why we use
Electronics Forum | Wed Sep 22 02:45:23 EDT 1999 | Brian
| | Dear All, | | | | In order to understand the soldering technologies in SMT, I'd like to understand why some cards are soldered and then cleaned, or only soldered whitout water cleaning nor "ultra sound" wavelength. | | | | I mean that I wonder