Skewed and popped components

Electronics Forum | Fri Sep 26 12:57:09 EDT 2003 | Angie

We have had some components that popped off in our IR oven. It was attributed to the solder paste. The humidity was above 60% the temp was about 70 degrees.

When? How and What??

Electronics Forum | Tue Aug 22 10:06:53 EDT 2000 | George English

Has there been a definite date for the total move over to lead free? Will it be 2004 or 2008. Also is there a direct replacement for leaded solder, I have read various articles on numerous alloys suggested for the switch, such as bismuth, tin, copper

Dye and Pry

Electronics Forum | Wed Mar 12 10:26:10 EDT 2008 | realchunks

Why would a board failure related problem be a process problem. I agree most companies believe EVERY problem is a Proces Problem, but in the real world we know this is not true. A pad lifting means your solder joint was able to rip it off the boa

Circuit cam and mydata

Electronics Forum | Fri Apr 10 10:20:15 EDT 2020 | unisoft

Yes process engineers that work for contract manufacturers try to get the full CAD or XY rotation files from their clients unfortunately still many of their customers still give them only Gerber files for the PCB project. Unisoft has had a focus on

Re: Paste-in_hole and CTE

Electronics Forum | Fri Jul 28 14:34:13 EDT 2000 | Gary Simbulan

Belive it or not, these boards were run through a Centech batch mode Vapor Phase machine. Single stage top side IR preheat. Vapor temp 218 C. Solder paste is an SN62 RMA.The boards were FR4 8 layer w/ solder mask, fairly conventional as might be e

Re: IPC and Nepcon

Electronics Forum | Wed Nov 18 14:42:22 EST 1998 | Dave F

| I heard somewhere that SMEMA has joined IPC, and that the association has decided to boycott Nepcon from | year 2000. Can anyone tell me if this is true | Nick: SMEMA and IPC are talking about merging (EP&P, 11/98, p 18). Below is a news release

Nitrogen and dry cabinet

Electronics Forum | Tue Jul 30 08:38:55 EDT 2002 | dasal

Truthfully, there are pro's and con's for both technologies. (put cost of ownership aside for one moment) Nitrogen won't dry humidified components as rapidly as a desiccant dry box. I'm talking about a self regenerating dry box that uses molecular s

IP1 and SSOP28

Electronics Forum | Tue May 18 21:43:02 EDT 2010 | ashley

Hello mickd, 1) The EL data & Vision_type is NOT necessary when using MCS30 for IP1 machine. note : your input of the above might have cause confusion during VP, hence the OS error. 2) I would suggest the following... 2a) lower the Lead_check_are

Manncorp Pick and Place

Electronics Forum | Tue Aug 05 21:08:10 EDT 2014 | isd_jwendell

You are correct about the Manncorp machine, it was an MDC machine. The Essemtec machine is old(ish) but still runs fine, and last I knew they were still supporting it. My recent problem with Essemtec was in regards to software. I found a bug and sim

Circuit cam and mydata

Electronics Forum | Wed Apr 15 18:37:15 EDT 2020 | unisoft

The point here is if you can't get the full CAD files or the XY rotation files and all you get his Gerbers and a BOM. Most all contract manufacturers and some OEM's at some time or another have to deal with Gerber only files. If you find yourself i

  1 2 3 4 5 6 7 8 9 Next

focus and ir searches for Companies, Equipment, Machines, Suppliers & Information

fluid dispenser

Stencil Printing 101 Training Course
Selective soldering solutions with Jade soldering machine

High Precision Fluid Dispensers
SMT feeders

World's Best Reflow Oven Customizable for Unique Applications
Pillarhouse USA for Selective Soldering Needs

Training online, at your facility, or at one of our worldwide training centers"


"回流焊炉"