Electronics Forum | Tue Apr 04 02:46:39 EDT 2000 | George Verboven
We are looking for a way to cure conductive adhesive. I heard about curing times from 2 hours and more. But I also received information that curing can be done in 10 minutes at 120 C. Of course it also depends from the type of glue. But the question
Electronics Forum | Wed Apr 05 22:42:28 EDT 2000 | Dave F
George: I would think so. We use an old Vitronics (822??) IR reflow oven to clue SMT adhesives. Gp get 'em!!! Dave F
Electronics Forum | Sun Jul 26 05:43:21 EDT 1998 | Amr Sokkary
Dear sirs, please help me to fing a company whicjh produces white or yellow adhesive UV curing glue for SMT components assembly ,i need names and contact fones and faxes for those company ,i need any company but not Alphametal or heraues thanks a
Electronics Forum | Mon Jul 27 21:05:36 EDT 1998 | Dave F
| Dear sirs, | please help me to fing a company whicjh produces white or yellow adhesive UV curing glue for SMT components assembly ,i need names and contact fones and faxes for those company ,i need any company but not Alphametal or heraues | th
Electronics Forum | Mon Jul 27 21:05:26 EDT 1998 | Dave F
| Dear sirs, | please help me to fing a company whicjh produces white or yellow adhesive UV curing glue for SMT components assembly ,i need names and contact fones and faxes for those company ,i need any company but not Alphametal or heraues | th
Electronics Forum | Tue Jul 28 10:59:07 EDT 1998 | Jose Moreno
| Dear sirs, | please help me to fing a company whicjh produces white or yellow adhesive UV curing glue for SMT components assembly ,i need names and contact fones and faxes for those company ,i need any company but not Alphametal or heraues | th
Electronics Forum | Tue Jul 28 10:55:54 EDT 1998 | Jose Moreno
| Dear sirs, | please help me to fing a company whicjh produces white or yellow adhesive UV curing glue for SMT components assembly ,i need names and contact fones and faxes for those company ,i need any company but not Alphametal or heraues | th
Electronics Forum | Mon Jul 27 12:24:29 EDT 1998 | Bill Schreiber
Ablestik 20021 Susana Rd. Compton, CA 90221 Tel: 1(310) 764-4600 Fax: 1(310) 764-2545 Grace 55 Hayden Ave. Lexington, MA 02173 Tel: 1(617) 861-6600 Fax: 1(617) 861-9590 Emerson Cumings makes a yellow. However, I do not have any contact info. Good luc
Electronics Forum | Sat Oct 06 08:36:04 EDT 2001 | davef
Your point about thermosets getting soft in the preheater of the wave is well taken. But an adhesive that is used past its expiry or other up-front lack of process control represent 99 & 44/100 percent of the reason for �glued parts falling off in
Electronics Forum | Fri Oct 05 07:46:24 EDT 2001 | george
Specifications of testing force are not fixed, but (incase of wave soldering) the value should be at least 120-150 % of the force the wave. So for small chip components we assume that the force from the wave on the component is about 3 Newton, this m