Electronics Forum | Wed Sep 07 17:14:11 EDT 2005 | GS

finest pitch requires ball bonding (gold) GS

wirebonding

Electronics Forum | Thu Sep 08 07:04:02 EDT 2005 | davef

Finer pitch: Wedge bonding can be designed and manufactured to very small dimensions, down to 50 mm pitch. Processing speed: Machine rotational movements make the overall speed of the wedge bonding process less than thermosonic ball bonding. Alumin

gold wire bonding

Electronics Forum | Thu Dec 29 10:47:05 EST 2005 | Chris

The paper Dave posted the link for is great. I have to go back and read it in depth. I can build prototypes by wirebonding to ENIG. I can do it on a manual wirebonder but I don't have the patience to do it on a magazine to magazine automatic machi

Wire bonding on gold fingers

Electronics Forum | Mon Aug 02 11:21:29 EDT 2004 | sforman1

Use MicroCoat Technologies UV cure solder mask. will leave PCB absolutely clean. used in many PCB solder/wirebonding apps. http://www.m-coat.com

Wire bonding on gold fingers

Electronics Forum | Mon Aug 02 11:44:49 EDT 2004 | jbabson1

If you do wire bond before printing, Photo Stencil (www.photostencil.com)can help you design a stencil with relief on the pwb side for the wirebonding.

Wire bonding on gold fingers

Electronics Forum | Tue Jul 01 17:38:24 EDT 2003 | jartman

I've faced this several times in the past, and the only real solution is to wirebond before SMT assembly. Everything leaves a residue, and trying to clean a residue off later is basically hopeless. This may require some trickery in your SMT process

soldering and bonding on gold PCB's

Electronics Forum | Wed Jan 09 18:17:15 EST 2002 | Chris

I don't have a plasma cleaner either. It will help a lot. Actually I don't clean at all. Our wirebond pads are far enough away so the flux residue does not get on the wirebond pads. That's what we think anyway. I am sure we have some degree of c

soldering and bonding on gold PCB's

Electronics Forum | Wed Jan 09 17:03:44 EST 2002 | rob_thomas

We follow IPC-2221 recommendations for Au and don't have a problem as long as the Ni is under 150 microinches.This ensures a consistent process for us.Also we do plasma clean after SMt and prior to wirebond.That makes a big difference. Rob

aluminium wire bonding on Electroless Nickel + Immersion gold

Electronics Forum | Tue Aug 21 22:24:36 EDT 2001 | davef

Root around here http://www.kns.com/resources/library/lib-wirebonding.asp

aluminium wire bonding on Electroless Nickel + Immersion gold

Electronics Forum | Mon Aug 27 15:06:29 EDT 2001 | davef

This otta push Wolfgang over the top ... Recommended reading G.G. Harman, Wire Bonding in Microelectronics : Materials, Processes, Reliability, and Yield, 2nd edition, McGraw-Hill Electronic Packaging and Interconnection Series, 1997. G.G. Harman, R

  1 2 3 Next

gold wirebonding searches for Companies, Equipment, Machines, Suppliers & Information

Win Source Online Electronic parts

Component Placement 101 Training Course
used smt parts china

Training online, at your facility, or at one of our worldwide training centers"
2024 Eptac IPC Certification Training Schedule

High Throughput Reflow Oven
2024 Eptac IPC Certification Training Schedule

World's Best Reflow Oven Customizable for Unique Applications