Re: Non soldered leads on ic's

Electronics Forum | Fri Feb 19 09:14:52 EST 1999 | Justin Medernach

| During inspection and test we find leads which do not get soldered. Some are because of insufficient paste, but with others everything looks right. This will only happen on 1 to 2 pins, and it is not isolated to a specific type of ic or location o

Solder joint strength

Electronics Forum | Mon Apr 04 17:32:07 EDT 2005 | toromaster

we also have a need to measure the solder bond strength of our gull wing parts on our pwb. there are many published comparisons between eutectic SnPb and no Pb solders out there. the number that comes to mind is about 10N to 15N. I have not looked

Qualitek Super Deox H

Electronics Forum | Wed Jan 16 16:42:45 EST 2008 | gsala

Hello, does anyone of you have experience by using Qualitek Super Deox H, dross reducer on Lead Free solder pot ? Any concern by using it ? Thank you Regards......GSx

SOLDER MASK PER ANSI/IPC-SM-840

Electronics Forum | Fri May 27 14:09:19 EDT 2022 | davef

No solder mask; Class 2 => Class T; Class 3 => Class H.

Manual soldering - solder wire diameter and soldering iron tip size for different component sizes

Electronics Forum | Tue Apr 16 05:05:32 EDT 2013 | stivais

We recently had a discussion with customer's QM - he claims that calculations for a proper solder wire diameter and soldering iron tip size (and temperature) have to be performed and documented for all manual (T/H) solderings (based on component size

Washable Soldermask on PWB

Electronics Forum | Mon Feb 02 11:52:07 EST 2009 | pjc

Is anybody using H2O washable solder mask that comes on the PWBs you get from the fab vendor? I am researching PWB vendors that can provide this service. Thanks.

Pasting a thru-hole part at SMT

Electronics Forum | Wed Dec 05 03:33:22 EST 2007 | longlee

We have done Paste-In-Hole process for 4 years.I think this prcess is suitable for 28-pins connector. Of course, you must assure the connecotr can endure high temperature firstly.Secondly, you need calculate the volume of solder paste, you can refere

popcorning in wave soldering

Electronics Forum | Tue Sep 12 04:48:26 EDT 2000 | Daniel

Is there a risk of popcorning plastic components during wave soldering? (The PCB is first surface mounted, reflowed and washed. It is sometimes left in air environment for as long as 48 h before the throgh hole components are mounted and they are wa

Blowholes during wave soldering

Electronics Forum | Mon Sep 03 06:17:19 EDT 2007 | mun4o

hi, This is moisture problem, I think.I have similar problem.You must try to bake PCBs.I bake our PCBs in solder wave mashine , under solder pot.There T is about 80*C - after 6-8h the PCB is dry regards

Wave Solder-Pallet

Electronics Forum | Fri Dec 03 18:04:52 EST 2021 | SMTA-64387687

Why don't you use peelable/washable solder mask on the SMT components next to the T/H pins? Then, you won't have to worry about keeping the tight tolerances.

  1 2 3 4 5 6 7 8 9 10 Next

h soldered searches for Companies, Equipment, Machines, Suppliers & Information

Void Free Reflow Soldering

High Resolution Fast Speed Industrial Cameras.
Sell Used SMT & Test Equipment

Nozzles, Feeders, Spare Parts - Siemens, Fuji, Juki, Yamaha, etc...
Voidless Reflow Soldering

High Throughput Reflow Oven
PCB Handling with CE

World's Best Reflow Oven Customizable for Unique Applications


"回流焊炉"