Electronics Forum: halogenated (Page 1 of 6)

Non-halogenated PCB

Electronics Forum | Wed Jul 19 11:06:42 EDT 2000 | polymer

Where can I find laminates containing non-halogenated PCB? I'm especially interested in FR-4 and CEM-3, 1.6 mm 25um. Thanks in advance! Dr. Lennart Johansson Polymer Support

Re: Non-halogenated PCB

Electronics Forum | Wed Jul 19 20:30:38 EDT 2000 | Dave F

Lennart: I think most laminators offer a halide free laminate. Two are Isola and Mica-Micanite. Contact the IPC Halogen-Free Materials Task Group

halogen free substrate

Electronics Forum | Tue Oct 29 11:20:17 EST 2002 | nifhail

Guys, Has anyone considered the specific use of Halogen free substrates for enhanced PCB performance? What is the impact on the PCB price ? Pls help.thank you in advance.

Dibasic Flux Activators

Electronics Forum | Wed Aug 23 09:12:54 EDT 2000 | Dave F

Dr. Lee: When talking about halogen-free flux activators, what does the term "dibasic" mean?

halogen free substrate

Electronics Forum | Thu Oct 31 11:23:32 EST 2002 | yngwie

Any input to my question ?

Rosin vs. Resin Flux

Electronics Forum | Thu May 31 12:21:14 EDT 2007 | patrickbruneel

Let me give you some good advice You take already plenty of risk going lead-free, DO NOT use halogen containing fluxes in a lead-free no-clean process. Halogens left on the board will convert tin, silver and exposed copper into metal salts over tim

Halogen-free Solder Re-flow Quality Issues

Electronics Forum | Tue Nov 03 09:49:08 EST 2015 | gregoryyork

how long are your squeegees for 3 - 5Kg pressure?

Halogen-free Solder Re-flow Quality Issues

Electronics Forum | Fri Nov 06 11:56:43 EST 2015 | derrikf

They're probably 12 - 18 inches, maybe slightly longer.

Water Absorption of PCB

Electronics Forum | Thu Feb 15 21:09:45 EST 2007 | Stephen- SMT engineer trainee

1. Can anyone tell me about the water absorption(wt%) among different PCB((i) RoHS, (ii)non-RoHS, (iii) Halogen free)), I am currently facing the problems of PCB blisters after reflow process. 2. Also, please suggest the baking period/time among dif

Halogen-free Solder Re-flow Quality Issues

Electronics Forum | Fri Sep 04 04:39:08 EDT 2015 | grahamcooper22

Maybe look at reducing the time above liquidus to @ 60 seconds. HF materials tend to want tighter reflow profiles...halogen activators are great at higher temps and longer reflow profiles..but HF prefer shorter profiles. The HF pictures look like the

  1 2 3 4 5 6 Next

halogenated searches for Companies, Equipment, Machines, Suppliers & Information

Circuit Board, PCB Assembly & electronics manufacturing service provider

World's Best Reflow Oven Customizable for Unique Applications
High Throughput Reflow Oven

High Precision Fluid Dispensers
Online Equipment Auction Jabil Monterrey MX Aug 19, 2024

Software for SMT placement & AOI - Free Download.
Hot selling SMT spare parts and professional SMT machine solutions

Private label coffee for your company - your logo & message on each bag!