Electronics Forum | Fri May 31 08:51:09 EDT 2002 | zanolli
Hello Dave, As related to connector mating interface, fretting corrosion is the oxidation of the contact points, causing high resistance across the interface. Fretting corrosion is caused my micromotions in the interface exposing the metalized conta
Electronics Forum | Fri May 31 17:04:02 EDT 2002 | davef
We use boots / shunts er wutt ever you call them to protect solderable component surfaces from wave soldering. Not sure how it would work in your case try: * Kinnarney Rubber 450 Main St. P.O.Box 37 Mantua, N.J. 08051 609-468-1320 fax 7438 http://ww
Electronics Forum | Tue Aug 26 09:30:56 EDT 2003 | Jim Z
Marc, There are many types of nylon used in the connector industry and some are designed to be used in high temperature (225-250C) oven reflow applications. These high temp nylons are usually types 4/6 and 6T. It sounds like you are either using a
Electronics Forum | Tue Aug 26 11:15:47 EDT 2003 | blnorman
We use HTN (high temperature nylon - Zytel) connectors in our reflow ovens with no warping, bubbling, or cracking. You can also use PPA (Amodel).
Electronics Forum | Mon Oct 25 17:06:18 EDT 1999 | William
Mario, If you are looking for a cheap press to do press fit connectors, then you are asking for trouble. Now, and in the long run. ASG out of West Palm Beach makes a very good press. We bought a 5 ton version and are able to press up to about 2500
Electronics Forum | Wed Dec 29 14:30:28 EST 1999 | Dan Woodward
I am not sure if I have seen an article comparing solder joint strength Vs pressfit although I am sure this has been researched by literally hundreds of companies before they felt comfortable going to pressfit. I know one of the issues with solder is
Electronics Forum | Mon Jul 22 09:53:13 EDT 2019 | kylehunter
Hey all! As background, I recently purchased a full SMT line for my company. We have a DEK 265, an assembleon opal xii, and a Heller 1500. Currently our jobs are leaded, and the heller is working perfectly. An upcoming job that we are potentially g
Electronics Forum | Wed Jul 06 15:26:12 EDT 2022 | glasscake
No experience with low temp solders for PIHR but we do use standard lead free 245-255 peak profiles on high temp connectors frequently. Honestly the added cost of the high temp connector pays for itself in labor. I almost always use oversized apertu
Electronics Forum | Thu Jun 30 12:21:33 EDT 2022 | kumarb
Thanks. Yes, we have attempted to use standard ROHS profiles in the past and turned our THT connectors into 'chucky dolls' after the PCBA left the oven. We then realized that we need the high temp nylon connectors to allow for the use inside the SMT
Electronics Forum | Fri Sep 06 03:06:18 EDT 2013 | 5pcb
We are a complex pcb supplier in China. We are good at making prototypes and multilayer (8-20)layers PCB. If you think your boards are difficult enough, you can contact me. Let's talk details. sales2@dmele.com Name:Lily Tel:0086-0755-23006293.