Electronics Forum | Thu Aug 27 11:35:07 EDT 2009 | davef
There are many possibilities: * Conformal coat is incompatible with surface residue on the board * Conformal coat is incompatible with solder mask on the board * Moisture is out-gassing from the board * Conformal coat is too thick and does not allow
Electronics Forum | Fri Apr 21 17:46:29 EDT 2006 | SD
First of all, do not use kapton tape! It tends to cause a dewetting effect around the tape. A call to Humiseal will explain why. There's not really a blanket answer to your question.... Removing cured liquid mask can often result in a fillet ef
Electronics Forum | Wed Jun 03 01:06:13 EDT 1998 | Mike Moninger
| We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not al
Electronics Forum | Tue Jun 02 14:32:58 EDT 1998 | Chris Fontaine
We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not alwa
Electronics Forum | Wed Jun 03 07:13:27 EDT 1998 | Tom Tellinghuisen
| We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not al
Electronics Forum | Tue Jun 02 15:53:32 EDT 1998 | Earl Moon
| We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not al
Electronics Forum | Wed Jun 03 15:22:12 EDT 1998 | Greg Curler
| | We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not
Electronics Forum | Tue Jun 02 17:36:43 EDT 1998 | Chris Fontaine
| | We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is not
Electronics Forum | Tue Jun 02 18:01:47 EDT 1998 | Earl Moon
| | | We have experienced poor adhesion of acrylic conformal coating to plastic bodied IC�s. The observed symptoms of this are a blistering or lifting of the coating at the surface of the component, although peel testing has revealed that this is no
Electronics Forum | Tue Jul 03 01:54:42 EDT 2018 | rdhiman1
Reaching out to all conformal coating experts, please help! While setting up conformal coating using the automated atomized spray, we observing issues associated with conformal coating wetting on the following regions: 1) Component edges 2) Metalli
The SMTA membership is a network of professionals who build skills, share practical experience and develop solutions in electronic assembly technologies and related business operations.
Training Provider / Events Organizer / Association / Non-Profit
6600 City W Pkwy
Eden Prairie, MN USA
Phone: 952-920-7682