Electronics Forum: how to braze copper to aluminium (Page 1 of 4)

to seal exposed copper layers

Electronics Forum | Fri Oct 20 14:13:32 EDT 2000 | DENNIS XIONG

Dear all, We have a PCB design mistake that causes exposed copper layers on the edges of breakaway locations. Although we fixed the design, but we already made a lot of boards plus many made before we found the problem. I wonder if any one have some

how to solder manganin 0.05mm manganin wire to a copper plate

Electronics Forum | Thu Jan 29 05:13:35 EST 2015 | neeraj_iiser

how to solder manganin 0.05mm manganin wire to a copper plate

how to solder manganin 0.05mm manganin wire to a copper plate

Electronics Forum | Fri Jan 30 00:41:04 EST 2015 | neeraj_iiser

Thanks a lot , my application is cryogenic in nature. I am trying to make a Sub-Angstrom resolution Thermal expansion sensor, whose components have been machined out of OHFC copper, and i needed to solder a manganin wire to one of the capcitor plates

how to solder manganin 0.05mm manganin wire to a copper plate

Electronics Forum | Thu Jan 29 09:18:36 EST 2015 | davef

Nichrome, manganin, phosphor bronze etc are easy to solder ... the hard part is removing the corrosion * Manganin: 86% copper, 12% manganese, 2% nickel. Often, it's used in making cryogenic measurements, due to its low heat loss. * Select a flux for

Water Residue Stains - how to remove?

Electronics Forum | Wed Dec 19 01:17:13 EST 2001 | ianchan

Hi Experts, I need help here, advice appreciated from all... Production is running a Lot of flex-circuit PCB, through the SMT line, with 0402 components. The flex-PCB is taped to FR4 support "pallets" when processing thru' the SMT P&P m/c. We use

Etch strain gauge in copper layer to measure deformations during press process [How to?]

Electronics Forum | Thu May 15 09:55:16 EDT 2014 | julianf

Tmo, Thanks for your reply. It gives good advise about how to perform tests. The type of strain gauges that I want to design are inside the PCB at various layers and I want to read the data during the press step. Do you know if these prefabricated

Etch strain gauge in copper layer to measure deformations during press process [How to?]

Electronics Forum | Fri May 16 05:17:13 EDT 2014 | julianf

Interesting. How did you connect the gauges in the press? Our press only has connections for thermocouples. But in essence, it's only a wire and an electical output. If you placed these prefabricated gauges on top and on the bottom surface, weren't

does copper wire become thinner when it dip to leadfree solder?

Electronics Forum | Thu Nov 03 04:31:21 EST 2005 | arnold

davef, how can you convince me that 100Sn dissolved copper much faster?

Etch strain gauge in copper layer to measure deformations during press process [How to?]

Electronics Forum | Wed May 14 13:31:22 EDT 2014 | taiji

You should look in to this document: IPC/JEDEC-9704A Printed Circuit Assembly Strain Gage Test Guideline Regards

Etch strain gauge in copper layer to measure deformations during press process [How to?]

Electronics Forum | Thu May 15 17:34:17 EDT 2014 | taiji

I always made tests with gauges on top or bottom surface of the PCB, before, during and after the process that we wanted to check. But I never tried to do it on internal layers of PCB. Don't know if that is possible. Regards

  1 2 3 4 Next

how to braze copper to aluminium searches for Companies, Equipment, Machines, Suppliers & Information

Circuit Board, PCB Assembly & electronics manufacturing service provider

Best Reflow Oven
best pcb reflow oven

Stencil Printing 101 Training Course
High Throughput Reflow Oven

Wave Soldering 101 Training Course
Win Source Online Electronic parts

Software programs for SMT placement and AOI Inspection machines from CAD or Gerber.
design with ease with Win Source obselete parts and supplies

Private label coffee for your company - your logo & message on each bag!