Electronics Forum | Thu Dec 18 15:48:25 EST 2003 | Subhash Nariani
Hello, Does anyone have experience with the PCB assembly of 0.5mm pitch chip scale packages with HASL finish? Characterization data that you can share? Tribal knowledge has it that the height variations of the solder prevent the use of HASL for fin
Electronics Forum | Thu Jan 12 11:06:27 EST 2006 | muse95
No not really. They are inspected with gloves, but all PCB's are in our facility, no matter what the finish. They are stored in the same packaging material that they are shipped in. We haven't been using ImmAg for that long yet, so maybe we will se
Electronics Forum | Tue Sep 02 16:07:04 EDT 2008 | blnorman
Colorization is relatively uniform across the board. "Processing" is first pass reflow. I belive MacDermid is the ImmAg supplier. Plating thickness has not been determined, our XRF is being revitalized. Elemental analysis did show a large copper
Electronics Forum | Mon May 14 13:33:36 EDT 2007 | jax
Solderability!!! The CM in question has probably seen too many solder problems with White Tin in the past. We have had the same issues. To save us from spending too much time and money(verifying pure Tin plating thickness, Chemical leaching from th