Re: Black spots on gold finish pads.

Electronics Forum | Tue Dec 01 07:54:49 EST 1998 | kallol chakraborty

| | Hi folks , | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Our inspec

Immersion white tin wave soldering problem

Electronics Forum | Fri Dec 16 08:00:26 EST 2005 | jax

What you are most likely dealing with: Insufficient Pure Sn layer ( multiple causes ) Because elevated temperatures accelerate the diffusion process, the thickness of the Pure Sn layer will reduce during every thermal cycle... ( bakeing PCBs, S

Re: wave solder process

Electronics Forum | Thu Jun 17 15:18:54 EDT 1999 | Earl Moon

| Does anyone know where I can find a list of things to do to when troubleshooting issues during the wave solder process? | | for example: | | Solder Bridge | 1.verify amount of flux been aplied. | 2.verify turbulance on your solder wave. | 3.etc.

Re: wave solder process

Electronics Forum | Thu Jun 17 19:52:57 EDT 1999 | Tony

| | Does anyone know where I can find a list of things to do to when troubleshooting issues during the wave solder process? | | | | for example: | | | | Solder Bridge | | 1.verify amount of flux been aplied. | | 2.verify turbulance on your solder w

Re: wave solder process

Electronics Forum | Thu Jun 17 20:35:51 EDT 1999 | Earl Moon

| | | Does anyone know where I can find a list of things to do to when troubleshooting issues during the wave solder process? | | | | | | for example: | | | | | | Solder Bridge | | | 1.verify amount of flux been aplied. | | | 2.verify turbulance on

Re: wave solder process

Electronics Forum | Mon Jun 21 14:55:27 EDT 1999 | JohnW

| | Does anyone know where I can find a list of things to do to when troubleshooting issues during the wave solder process? | | | | for example: | | | | Solder Bridge | | 1.verify amount of flux been aplied. | | 2.verify turbulance on your solder w

Re: Black spots on gold finish pads.

Electronics Forum | Tue Dec 01 09:02:18 EST 1998 | Earl Moon

| | | Hi folks , | | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Our in

Re: Black spots on gold finish pads.

Electronics Forum | Fri Dec 04 20:26:34 EST 1998 | kallol Chakraborty

| | | | Hi folks , | | | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most. Ou

Re: Black spots on gold finish pads.

Electronics Forum | Fri Dec 04 20:37:45 EST 1998 | kallol chakraborty

| | | | | Hi folks , | | | | | Lately we are seeing a lot of rawcards with black spots on the pads - most of them have Au finish(immersion gold) . We did a lot of inspecton after wave solder and found that only (fine pitch) QFP are affected the most

Brush-Up Your Intermetalics!!!

Electronics Forum | Thu Jun 17 21:31:06 EDT 1999 | Dave F

| | Does anyone know where I can find a list of things to do to when troubleshooting issues during the wave solder process? | | | | for example: | | | | Solder Bridge | | 1.verify amount of flux been aplied. | | 2.verify turbulance on your solder w


immersion depth searches for Companies, Equipment, Machines, Suppliers & Information



High Resolution Fast Speed Industrial Cameras.
Selective Soldering Nozzles

Easily dispense fine pitch components with ±25µm positioning accuracy.
High Throughput Reflow Oven

High Throughput Reflow Oven
PCB Handling with CE

World's Best Reflow Oven Customizable for Unique Applications
Fully Automatic BGA Rework Station

"回流焊炉"