Electronics Forum | Wed Aug 15 16:04:23 EDT 2001 | davef
First, responding to your question � Several things on copper dissolution in solder are: * A 50um copper wire will dissolve in 60Sn / 40Pb solder at: - 200�C solder in 55 seconds; - 250�C solder in 20 seconds; - 300�C solder in 5 seconds; - 350�C so
Electronics Forum | Fri Aug 30 02:12:19 EDT 2013 | raqz
Hi! I have been studying the reflow process. And now, I am researching for a recommended reflow oven that can process a small to low-medium production SMT soldering. For the experts in the reflow field, please recommend a reliable reflow oven. Here
Electronics Forum | Fri Nov 12 13:07:45 EST 2010 | G8reflow
Hi, The focal point of my research has been to recommend a reflow oven and develop a process for a small to low-medium production SMT soldering with the following considerations. - Lead-Free - Low to low-medium production - Forced Convection reflow