Electronics Forum | Wed Dec 22 11:12:33 EST 2004 | Steve
Does anyone have an opinion about the pro's and con's of Getek vs Isola FR408 laminate? What laminate to most of you call out? Thanks in advance for your feedback. Steve
Electronics Forum | Fri Oct 27 11:17:41 EDT 2006 | MFG CAVEMAN
Since I didn't see it mentioned - Are you specifying a laminate that is considered compatible with a RoHS process? I don't mean just a high Tg but a high Td (decomposition) and CTE material such as Isola 410, FR408 etc.
Electronics Forum | Fri Oct 27 13:58:27 EDT 2006 | markb
We use the Isola 410 laminate. They just issued a tech bulletin on the same day (coincidence???) that we found the problem. It mostly talks about handling (i.e. environmental storage) and pre-bake operations to prevent issues like this.
Electronics Forum | Thu May 08 12:11:30 EDT 2008 | boardhouse
Hi Wayne, I am just curious what material is being called out. Are you just specing FR4 or are you calling out a particular IPC 4101 / Some recommended laminates designed for Lead free assembly are: Isola 370HR Nelco 4000-11 or 4000-29 Iteq IT15
Electronics Forum | Thu Jan 31 18:14:40 EST 2008 | boardhouse
Hi Felix, First thing to verify is that your supplier is actually suppling you with the correct material. China is known for not keeping with the requested materials and will substitute if not controlled. I would recomend ITEQ, TUC or Nan ya for of
Electronics Forum | Tue Jul 31 15:33:30 EDT 2007 | gregs110
I have seen a few threads about delamination issues on IS410 laminate in RoHS applications. I have recently been running into a rash of issues on 4 different part numbers with a single PWB source. All the parts have been built fine in the past with
Electronics Forum | Mon Dec 08 17:06:59 EST 2008 | boardhouse
Hi MGL, Couple things to ask, have the boards recently been changed to Rohs builds? STD FR4 to High TD Laminate. Check the stack-up the board houses are using. Just about all Rohs laminate has Resin starvation issues when used in single ply co
Electronics Forum | Wed Sep 10 02:47:49 EDT 2003 | Dennis O'Donnelll
This is a problem of contamination in the plating bath. Most prominent with white tin and some gold over nickel plating processes. Rather than argue with your vendor over the issue, and to avoid future recurring problems, I use either HASL or elect
Electronics Forum | Thu Sep 01 18:53:08 EDT 2005 | Board House
Pr. I agree with some of the above responses. if you are seeing Delam issues with incoming PCB's the following should be check. 1) Check the OEM Print to what Material they are calling out to be manufactured with. 2) If they are calling out for S
Electronics Forum | Tue May 12 12:28:22 EDT 1998 | Rin Or
| I'm in the process of doing an evaluation fora big board machine. My choices are Universal HSP 4791 and Fuji CP6-5. | Has anyone one a subjective evaluation on both machines? If so what was the outcome, abd experiences since installing the selected